Glossary

Rate-Controlled Sintering (RCS)

The properties of sintered products, such as DensityThe mass density is defined as the ratio between mass and volume. density or particle size distribution, are determined by the SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering conditions (temperature, atmosphere, etc.) and especially by the SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering rates. 

The NETZSCH Proteus® RCS software allows for control of this SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering rate during a dilatometer measurement. In contrast to a conventional dilatometer measurement where the length change of a sample is measured after following a given temperature program – usually under a constant heating rate – RCS determines the required temperature profile for a given rate of change in length. With RCS, the temperature program of the furnace is controlled so as to achieve predefined SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering rates for the sample. Depending on the selected RCS mode, the furnace may no longer be heated at a fixed rate. The heating process may be stopped/started or continuously adapted depending on the SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering rate of the sample. The measured temperature profile can then be used for optimizing the production process.

Example:
Alumina Green Body

A test run under RCS conditions on an alumina green body is shown here. The heating rate in the SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering range is reduced by the RCS control so as to achieve a nearly constant shrinkage rate. After the SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering process is finished, the heating rate returns to the programmed value.

Graphical analysis of rate-controlled sintering (RCS) for alumina green body, showcasing temperature profiles and shrinkage rates.

Do you have any questions?

Our experts will be happy to help you. 

Contact us

Suitable products for your measurement

AI Overview
An error occurred. Please try again.