04.07.2022 by Aileen Sammler

TBB 913 – Fire Testing System for Floor Coverings

A burnt cigarette rests on a carpet, revealing scorch marks and stains, highlighting the importance of fire-resistant floor coverings.

Ideally, fires should be directly prevented or the spread of flames should be contained as well as possible, for example, by using appropriate floor coverings. With the TBB 913 fire testing system for floor coverings by NETZSCH TAURUS Instruments, the fire behavior can be determined in order to classify floor coverings into the appropriate fire protection classes.

In protecting life and limb to the greatest extent possible in the event of a fire, the time factor from ignition to the arrival of emergency services plays a decisive role.

Fire-protection classes for floor coverings according to DIN EN 13501-1, highlighting flammability and safety standards.
Figure: Fire-protection classes for floor coverings in accordance with DIN EN 13501-1 (Source: https://www.cobaeurope.com/de/newsroom/ ratgeber-brandschutzklassen-fuer-bodenbelaege-nach-en-13501-1254

Particularly in public facilities like airports, hospitals, child-care centers, schools and hotels, but also in shipping, aviation and in the private sector, it is extremely important to comply with fire-protection requirements. For the building materials industry, the fire behavior in terms of flammability, flame spread and smoke development of the materials employed is of particular importance.

But how does one know whether the floor coverings employed meet fire-safety regulations? The DIN EN ISO 9239‐1 standard, which is valid throughout Europe, stipulates mandatory tests for the fire behavior of floor coverings along with the classi­fication of fire properties. With the new TBB 913 fire testing system for floor coverings by NETZSCH TAURUS Instruments, the fire behavior can be deter­mined in order to classify floor coverings into the appropriate fire protection classes.

TBB 913 fire testing system for floor coverings, designed to assess fire behavior and classify materials for safety regulations.
Figure: TBB 913 fire testing system

Functional Principle of the TBB and Classification into Fire Classes

The TBB 913 is used to simulate typical fire scenarios, which can occur, for example, in long corridors in hotels and public facilities. A heat radiator in an inclined position generates the high thermal radiation energy on the flooring occurring in the event of a fire. The flooring specimen to be tested is laid out horizontally in the test chamber. The flame propagation distance, the smoke DensityThe mass density is defined as the ratio between mass and volume. density as a function of time and the critical thermal radiation are determined.

For tests that can be used for purposes of comparison and drawing conclusions, high repro­ducibility is required. The heat-flux profile needed for the specimen must be detected and precisely adhered to within narrow limitations in accordance with the standard.

For determination of the smoke gas DensityThe mass density is defined as the ratio between mass and volume. density, trans­mission measurements (TRDA) along with temper­ature and pressure loss measurements are necessary to detect the gas volume flow. The gas velocity in the flue gas exhaust is also measured and constantly adjusted via speed-controlled fans. All types of floor coverings, such as carpets, wood, cork or plastic coverings, can be tested.

Combustion chamber of the TBB 913 fire testing system, featuring flames testing floor coverings for fire behavior and safety standards.
Figure: Combustion chamber with tiltable radiator of the TBB 913

Commercial and contract floor coverings employed in public or commercial buildings are tested in accor­dance with DIN EN ISO 9239‐1 and EN 13501‐1 for classification into the fire classes A1fl to Ffl.  Floor coverings are considered flame-retardant if they meet with the requirements associated with the radiation test for fire classes Bfl and Cfl. For products used in private homes, class Efl is usually sufficient.

Intuitive Operation Based on Windows

The TBB 913 fire testing system operates via the “TBB Control” measurement and control unit. The integrated software serves for recording and processing the measured values and displaying the measurement results in various formats.

Screenshot of TBB 913 software displaying real-time fire testing measurements for floor coverings, including temperature graphs and test parameters.
Figure: Screenshot of the measurement course with the Windows-based TBB software

Further details can be found on our website at https://analyzing-testing.NETZSCH.com/en/products/fire-testing/tbb-913