Glossary

Pyrolytic Carbon

Pyrolytic carbon is carbon which is generated by the PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis of organic matter in an oxygen-free atmosphere.  

Pyrolytic carbon can be quantified via TGA. Once PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis concludes in a nitrogen atmosphere, the gas atmosphere in the thermal analyzer is switched to air or oxygen. The pyrolytic carbon that was generated is burned and released as CO2. This mass loss can be recorded by means of TGA.

The figure below shows the PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis of polyvinyl alcohol in a nitrogen atmosphere and the subsequent burning of the pyrolytic carbon in an air atmosphere. The change in the gas atmosphere was carried out at 800°C. The pyrolytic carbon portion amounted to 3.9%. These kinds of studies are carried out mainly for polymers and can only be done on samples which do not already contain Carbon BlackTemperature and atmosphere (purge gas) affect the mass change results. By changing the atmosphere from, e.g., nitrogen to air during the TGA measurement, separation and quantification of additives, e.g., carbon black, and the bulk polymer can become possible.carbon black in the form of a filler, dye or carbon fiber reinforcement.

Measurement conditions: RT–800°C, nitrogen atmosphere 40 ml/min, 800°C–1000°C, air atmosphere 40 ml/min, heating rate 10 K/min, sample mass 10 mg

Graph displaying DTG and TG analysis of polyvinyl alcohol under nitrogen and air atmospheres, with temperature markers and percentage changes.