General Properties
Short Name: ASA
Name: Acrylonitrile-Styrene-Acrylate Copolymer
Acrylonitrile-styrene-acrylate copolymer (ASA) like ABS (see previous example) is also a terpolymer of three monomer units and has similar properties, but is more weather-resistant. ASA can be referred to as SAN-Polymer when acrylic ester is evenly distributed throughout the polymer.
Structural Formula

Properties
NETZSCH Measurement

| Sample Mass | 11.40 mg |
| Heating Rates | 10 K/min |
| Crucible | Al, pierced lid |
| Atmosphere | N2 (50 ml/min) |
Evaluation
Two Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.glass transitions can be seen in the above DSC curves. The first Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.glass transition can be attributed to the acrylate component and occurs in the 2nd heating at -50°C (midpoint, red curve) with a change in specific heat of 0.04 J/(g.K)). The second Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.glass transition is due to the styrene component. The larger the RelaxationWhen a constant strain is applied to a rubber compound, the force necessary to maintain that strain is not constant but decreases with time; this behavior is known as stress relaxation. The process responsible for stress relaxation can be physical or chemical, and under normal conditions, both will occur at the same time. relaxation peak, the more positively shifted the Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.glass transition temperature to higher temperatures, as in this example.