Highlights

Guarded Hot Plate - The Absolute Method for Testing Insulation Materials

Insulation materials are growing in significance in a number of applications, including the insulation of buildings. Improved insulation reduces energy use and consequently heating costs for each individual household or industrial operation.

The NETZSCH GHP 456 Titan® is the ideal tool for researchers and scientists in the field of insulation testing. Based on the well‐known, standardized guarded hot plate technique, the system features unrivaled performance over an unmatched temperature range. 

The GHP principle is based on an absolute measurement method and therefore requires no calibration standards. Combining cutting‐ edge technology with the highest quality standards, NETZSCH has designed a robust and easy‐to‐ operate instrument, featuring unparalleled reliability and optimum accuracy over a wide temperature range.

Advanced industrial testing equipment featuring a stainless steel chamber mounted on a robust electronic control unit.

The Guarded Hot Plate is an absolute method

The great advantage of the GHP method is that it is an absolute method; i.e., no calibration or correction is required at all. The Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity values result in the stationary state simply from the: 

  •  precisely measured total power input into the hot plate, Q
  • average sample thickness, d,
  • measurement area, A, and
  • mean temperature difference, ΔT, along the sample or the two samples, as the case may be (the factor 2 results for two samples).
GHP 456 Titan apparatus in open position, showcasing hot and cold plates and additional components for material testing.
GHP 456 Titan® in open position. The samples are placed between the hot plate (1) with guard ring (2) and the lower (3) and upper cold plates (4), respectively. Additionally shown are the three‐part sectional furnace (5), insulation (6), feed‐throughs (7), hoisting device (8), and gas connection (9).

Guarded Hot Plate - Principle of Operation 

The hot plate and the guard ring are sandwiched between two samples of the same material and approximately the same thickness, d. Cold plates are placed above and below the samples. All plate temperatures are controlled such that a well‐ defined, user‐selectable temperature difference, ΔT, is established between the hot and the cold plates – and thus across the sample thickness. The guard ring is maintained exactly at hot plate temperature in order to minimize lateral heat losses.

NETZSCH offers more exciting products that support you in measuring Thermal Conductivity:

  • TCT 716 Lambda
    TCT 716 Lambda

    Determine the thermal conductivity of round solid specimens in the low- and medium-conductivity range with our Guarded Heat Flow Meter:

    • Sample mean temperature range: -10°C to 300°C
    • Thermal conductivity range: 0.1 … approx. 30 W/(m·K)
    • Two independent test stacks to measure two samples at the same time

     

  • HFM 446 Lambda Small Eco-Line
    HFM 446 LambdaSmall Eco-Line

    An exact, fast and easy-to-use instrument for measuring the low thermal conductivity, λ, of insulation materials.

    • Thermal conductivity range: 0.007 to 2 W/(m·K)
    • Metering area heat flux transducer: 102 mm x 102 mm
    • Specimen sizes (max.): 203 mm x 203 mm x 51 mm
  • TDW 4240
    TDW 4240

    Hotbox Test Chamber for testing construction materials (windows, profiles, doors, domes, brick walls etc.)

    • Measuring Range: R: 0.10 to 8.00 m²·K/W, U: 0.12 to 3.70 W/(m²·K)
    • Specimen thickness (H): up to 560 mm
  • LFA 717 HyperFlash
    LFA 717 HyperFlash®

    A fast, non-contact method for determining thermal diffusivity

    • Temperature range: -100°C to 500°C
    • Simultaneous measurement of up to 16 samples
    • Broadest sample holder and sample material range

Specifications

 GHP 456 Titan®
Technique/Design
  • Absolute method (no calibration or reference materials required)
  • Symmetrical arrangement
  • Fully automated operation
StandardsBased on standards such as ISO 8302, ASTM C177, DIN/EN 12667, DIN/EN 12939, etc
Mean specimen temperature range
  • Low‐temperature version: ‐160°C to 250°C
  • High‐temperature version: ‐160°C to 600°C 

Both versions require LN2 cooling for the sub‐ambient temperature range

Cooling systems

Liquid nitrogen (LN2): ‐160°C to 250°C

Compressed air: 50°C to 300°C

Chiller: 20°C to 85°C 

→ No active cooling from 300°C to 600°C

Plate dimensions
  • 300 mm x 300 mm
  • Motorized plate hoist
Plate material
  • Low‐temperature version: Aluminum alloy
  • High‐temperature version: Tungsten alloy
Plate temperature range
  • Standard version: ‐180°C to 270°C
  • High‐temperature version: ‐180°C to 620°C
Vacuum‐tightnessBy design, 5 x 10‐4 mbar (0.05Pa)
Defined pressure levelsControlled between 0.1 mbar and 100 mbar
Specimen thickness
  • Up to 100 mm (typically 10 ... 50 mm)
  • Max. difference in thickness for the two specimens to be measured: 2%
Atmosphere/ pressure level
  • Oxidizing up to 300°C
  • Inert
  • Vacuum
  • Defined pressure levels
Thermal conductivity range0.003 to 2 W/(m·K)*
Minimum measurable thermal resistance0.02 m2·K/W*
AccuracyTypically 2%*
ReproducibilityTypically < 1%*
Software specialties

SmartMode, including:

  • Method‐based, easy operation (e.g., user and predefined methods)
  • Support of controlled, adaptive cooling
  • Report generator
  • Results including combined standard uncertainties according to GUM**

* Depending on the measurement conditions and specimen properties 
** GUM = Guide to the Expression of Uncertainty in Measurement

GHP 456 Titan® – Technology

The vacuum-tight GHP 456 Titan® combines the latest developments in material science and electronics with state-of-the-art design and technology.

NETZSCH thermal analysis equipment with control monitor, used for material testing and analysis in research and development.

Accessories

  • Various pump systems (rotary pumps, turbo molecular pumps) are available for the GHP 456 Titan®. The system can be easily extended later on by add the appropriate pump to the connections of the system.
  • Standard materials: Various kinds of certified (NIST, NPL) standard materials (fiber insulations, foam insulations) are available for the system.
  • Cooling of the heat sinks: The heat sinks can be cooled with forced air (for mean sample temperatures above 40°C) with a chiller (for mean sample temperatures above 0°C) or with liquid nitrogen. The liquid nitrogen is supplied from a feeding system via a software controlled supply system.
  • For measurements of powders and flakes special calcium silicate frames are available, fitting exactly to the plate dimensions.
Customer support representative at a computer, smiling and engaged, highlighting NETZSCH's commitment to service excellence.


Proven Excellence in Service

At NETZSCH Analyzing & Testing, we offer a comprehensive range of services globally to ensure the optimal performance and longevity of your thermoanalytical equipment. With a track record of proven excellence, our services are designed to maximize the effectiveness of your devices, extend their lifespan, and minimize downtime. 

Unlock the full potential of your equipment with our tailored solutions, backed by years of industry expertise and innovation.

Software

All software highlights at a glance

NETZSCH GHP 456 software interface displaying sensor temperatures, setup options, and instrument information.

The Highlight of Proteus® Software - SmartMode

The convenient SmartMode allows for the prompt start of a measurement via Wizard, via methods which were defined by the user beforehand (known as User Methods), or via Predefined Methods supplied for the NIST 1450D, IRMM 440 and SilCal1100 standard reference materials. 

Integrated Stability Criteria Management

When should the measurement points be recorded? The Stability Criteria Manager within the Setup & Control section of SmartMode allows conditions to be defined before a measurement starts and even while it is in progress. The stability criteria ensure optimum reliability and reproducibility for the test results. Of course, the default stability criteria of the instrument work well for most specimens

NETZSCH GHP 456 software interface showing stability criteria settings, including temperature ranges and deviation measurements.

Related Devices

  • GHP 721-500 mm
    GHP 721-500 mm

    Guarded Hot Plate with touch display - especially for thick specimens

    • Measuring range: 0.005 to 2.0 W/(m·K), depending on material and thickness
    • Specimen size (L x W): 500 mm x 500 mm, variable, according to the dimension of the hot plate: 200 mm x 200 mm up to 300 mm x 300 mm
  • GHP 721-600 mm
    GHP 721-600 mm

    Guarded Hot Plate with touch display – for specimen dimensions up to 600 mm x 600 mm 

    • Measuring range: 0.005 to 2.0 W/(m·K), depending on material and thickness
    • Specimen size (L x W): 600 mm x 600 mm
    • dimension of the hot plate: 300 mm x 300 mm
  • GHP 456 Titan
    GHP 456 Titan®

    Innovative Guarded Hot Plate System GHP 456 Titan® for Determination of Thermal Conductivity of Insulations

    • Sample thickness: up to 100 mm (typically 10 ... 50 mm)
    • Temperature range: -160 to 250°C (low-temperature version) or -160 to 600°C (high-temperature version)
Formula 1 pit crew servicing a red racing car, showcasing teamwork and speed during a high-pressure race scenario.

Consultancy & Sales

Do you have further questions about the instrument or the method and would like to speak to a sales representative?

Service & Support

Do you already have an instrument and need technical support or spare parts?

Downloads and Media

AI Overview
An error occurred. Please try again.