GHP 456 Titan®
Innovative Guarded Hot Plate System GHP 456 Titan® for Determination of Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.Thermal Conductivity of Insulations
Highlights
Guarded Hot Plate - The Absolute Method for Testing Insulation Materials
Insulation materials are growing in significance in a number of applications, including the insulation of buildings. Improved insulation reduces energy use and consequently heating costs for each individual household or industrial operation.
The NETZSCH GHP 456 Titan® is the ideal tool for researchers and scientists in the field of insulation testing. Based on the well‐known, standardized guarded hot plate technique, the system features unrivaled performance over an unmatched temperature range.
The GHP principle is based on an absolute measurement method and therefore requires no calibration standards. Combining cutting‐ edge technology with the highest quality standards, NETZSCH has designed a robust and easy‐to‐ operate instrument, featuring unparalleled reliability and optimum accuracy over a wide temperature range.

The Guarded Hot Plate is an absolute method
The great advantage of the GHP method is that it is an absolute method; i.e., no calibration or correction is required at all. The Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity values result in the stationary state simply from the:
- precisely measured total power input into the hot plate, Q
- average sample thickness, d,
- measurement area, A, and
- mean temperature difference, ΔT, along the sample or the two samples, as the case may be (the factor 2 results for two samples).
Method
Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.Thermal Conductivity - A Key Parameter for Improved Energy Efficiency

Guarded Hot Plate - Principle of Operation
The hot plate and the guard ring are sandwiched between two samples of the same material and approximately the same thickness, d. Cold plates are placed above and below the samples. All plate temperatures are controlled such that a well‐ defined, user‐selectable temperature difference, ΔT, is established between the hot and the cold plates – and thus across the sample thickness. The guard ring is maintained exactly at hot plate temperature in order to minimize lateral heat losses.
- How is a particular insulation material performing?
- How can cryo tanks be insulated in the best possible way?
- Does cryogenic insulation reliably prevent heat exchange?
- What is the optimum insulation for furnaces operating under different temperature, gas or pressure conditions?
- Is the Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity low enough to prevent thermal bridges?
The GHP 456 Titan® is based on various relevant standards, e.g., ISO 8302, ASTM C177 or DIN EN 12667.
NETZSCH offers more exciting products that support you in measuring Thermal Conductivity:
Specifications
| GHP 456 Titan® | |
|---|---|
| Technique/Design |
|
| Standards | Based on standards such as ISO 8302, ASTM C177, DIN/EN 12667, DIN/EN 12939, etc |
| Mean specimen temperature range |
Both versions require LN2 cooling for the sub‐ambient temperature range |
| Cooling systems | Liquid nitrogen (LN2): ‐160°C to 250°C Compressed air: 50°C to 300°C Chiller: 20°C to 85°C → No active cooling from 300°C to 600°C |
| Plate dimensions |
|
| Plate material |
|
| Plate temperature range |
|
| Vacuum‐tightness | By design, 5 x 10‐4 mbar (0.05Pa) |
| Defined pressure levels | Controlled between 0.1 mbar and 100 mbar |
| Specimen thickness |
|
| Atmosphere/ pressure level |
|
| Thermal conductivity range | 0.003 to 2 W/(m·K)* |
| Minimum measurable thermal resistance | 0.02 m2·K/W* |
| Accuracy | Typically 2%* |
| Reproducibility | Typically < 1%* |
| Software specialties | SmartMode, including:
|
* Depending on the measurement conditions and specimen properties
** GUM = Guide to the Expression of Uncertainty in Measurement
GHP 456 Titan® – Technology
The vacuum-tight GHP 456 Titan® combines the latest developments in material science and electronics with state-of-the-art design and technology.
Two versions of the GHP 456 Titan® exist for the investigation of insulating materials, e.g., cryogenic insulation or insulation of hightemperature-furnaces. The instruments cover an extremely broad temperature range; however, the actual minimum achievable working temperature depends on the cooling system used.
Various cooling options are available for the system including pressurized air which allows for measurements at temperatures as low as 50°C and a chiller which permits 20°C. The liquid nitrogen (LN2) system enables measurements down to ‐160°C (minimal mean sample temperature each). The cooling strength is automatically minimized for best accuracy and reproducibility.
This makes the instrument to the ideal tool for researchers and quality control engineers across a broad field of high‐ performance insulation materials.
Plates made of aluminum and tungsten alloy are used to cover a temperature range of up to 250°C and 600°C, respectively. Each plate, the guard ring and the furnace are connected to a separate control system and stabilized power supply, ensuring fast attainment of programmed plate temperatures and perfect stability. In equilibrium, differences between the programmed and actual plate temperatures are ≤ 0.01 K for the hot plate and the guard ring.
The system is fully symmetrical. Usually, the measurement is carried out with two identical specimens for best accuracy. However, it is also possible to perform measurements with only one specimen. According to the relevant standards, this arrangement ensures the maximum possible accuracy of better than 2% at room temperature for most materials
A defined environment surrounds the entire plate stack. This sectional furnace (see also schematic on page 3) creates a temperature profile around the plate stack similar to what is generated by the plate stack itself. This nearly eliminates radial heat losses. Furthermore, all wiring to the plates is connected to the defined environment. Therefore, wire heat loss is negligible.

Accessories
- Various pump systems (rotary pumps, turbo molecular pumps) are available for the GHP 456 Titan®. The system can be easily extended later on by add the appropriate pump to the connections of the system.
- Standard materials: Various kinds of certified (NIST, NPL) standard materials (fiber insulations, foam insulations) are available for the system.
- Cooling of the heat sinks: The heat sinks can be cooled with forced air (for mean sample temperatures above 40°C) with a chiller (for mean sample temperatures above 0°C) or with liquid nitrogen. The liquid nitrogen is supplied from a feeding system via a software controlled supply system.
- For measurements of powders and flakes special calcium silicate frames are available, fitting exactly to the plate dimensions.
Brochures and Data Sheets:

Proven Excellence in Service
At NETZSCH Analyzing & Testing, we offer a comprehensive range of services globally to ensure the optimal performance and longevity of your thermoanalytical equipment. With a track record of proven excellence, our services are designed to maximize the effectiveness of your devices, extend their lifespan, and minimize downtime.
Unlock the full potential of your equipment with our tailored solutions, backed by years of industry expertise and innovation.
Software
All software highlights at a glance

The Highlight of Proteus® Software - SmartMode
The convenient SmartMode allows for the prompt start of a measurement via Wizard, via methods which were defined by the user beforehand (known as User Methods), or via Predefined Methods supplied for the NIST 1450D, IRMM 440 and SilCal1100 standard reference materials.
Integrated Stability Criteria Management
When should the measurement points be recorded? The Stability Criteria Manager within the Setup & Control section of SmartMode allows conditions to be defined before a measurement starts and even while it is in progress. The stability criteria ensure optimum reliability and reproducibility for the test results. Of course, the default stability criteria of the instrument work well for most specimens

SmartMode offers convenient, easily accessible report generation in accordance with GHP standards. It allows users to select between either a quick overview of the measurement results, including combined standard uncertainties (GUM), or a full report including comprehensive diagnostic information on the instrument and the measurement parameters. Of course, the reports can be adapted to one’s own corporate identity (CI)

The GHP software comes with a 32‐/64‐bit Windows operating system and allows for connection to a touch screen, keyboard and mouse and the use of a toolbar with shortcut buttons.
In the Idle Mode Setup, you can control the temperature of the plates and the chiller as well as the vacuum level of the instrument (additional equipment required).
The instrument comes with predefined methods for the NIST SRM 1450D, IRMM 440 and SilCal1100 reference materials. For each method, the temperature program and all other measurement parameters are already defined. In addition, operators can define their own methods, which are available under the User Methods menu.
The software can optionally be operated in the German, English, French, Russian*, Chinese* or Japanese* language.
* Russian, Chinese and Japanese languages can only be used if the necessary fonts are installed.
The wizards provide a measurement framework which considerably simplifies any additional definition of a measurement. Cooling devices, controlled vacuum, setpoint temperatures and time limits can all be programmed, depending on your measurement task
Related Devices

Downloads and Media
Application Literature
Our latest blog articles
- 21.01.2026
The Guarded-Hot-Plate Method: How Gas Type and Pressure Can Change the Thermal Conductivity of Your Insulation Materials

- 28.05.2025
Contract Testing of Thermophysical Properties – Enhanced with the NETZSCH TCT 716 Lambda Guarded Heat Flow Meter

- 21.11.2024
Measuring Thermophysical Properties with Focus on Thermal Conductivity

- 07.08.2024
NETZSCH TCT 716 Lambda: Der geschützte Wärmestrommesser zur direkten Messung der Wärmeleitfähigkeit