NETZSCH LFA 717 HyperFlash, a compact thermal conductivity analyzer designed for precise material testing and analysis.
Laser/LIght FLash Analysis

LFA 717 HyperFlash®

Light Flash Apparatus

Highlights

FOR HIGHLY ACCURATE AND FAST THERMAL DIFFUSIVITY MEASUREMENTS

The LFA 717 HyperFlash® is a state-of-the-art instrument designed to accurately measure the Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.thermal diffusivity of various materials. With its advanced calculation models, it is at the forefront of scientific innovation, ensuring accurate results essential for materials analysis.

Broad sample range: The LFA 717 HyperFlash® can accommodate a wide range of sample materials, including both round and square-shaped specimens. It features an automatic sample changer that can handle up to 16 samples simultaneously, increasing laboratory efficiency.

Flexible temperature control: The instrument offers remarkable flexibility in selecting the measurement range up to 500°C. Using liquid nitrogen, it can analyze samples at temperatures as low as -100°C. In addition, a compressed air unit allows subambient measurements down to 0°C. The integrated evacuation system permits measurements in defined atmospheres.

Advanced corrections specifically for thin or highly conductive samples: The latest version of our analysis software introduces an enhanced analysis pulse correction feature designed for high-precision applications where exceptional time resolution is critical. This enhancement is particularly beneficial when analyzing thin or highly conductive samples, and in situations where the light pulse coincides with the thermal response of the sample.

The LFA 717 HyperFlash® is an essential tool for researchers and industries requiring precise thermal property measurements, making it an invaluable asset in the field of materials science.

Please accept Marketing Cookies to see that Video.

Explore our LFA Webinar Series

Our webinar series brings you practical, application-focused sessions on LFA. Learn directly from NETZSCH experts and discover new ways to enhance your daily thermal analysis work.

View Full Series
Close-up of a sleek gray and silver testing device with labeled sections A, B, C, D, suitable for analytical applications.

The top cover of the instrument serves as a convenient area for sample preparation and storage. It has been thoughtfully designed with four visually distinct sections, each corresponding to specific specimen locations within the furnace. This innovative layout simplifies sample identification and pre-assembly, minimizes instrument downtime, and is especially beneficial in multi-user environments.

Method

Efficient Determination of Thermophysical Properties with the Light Flash Method

The Light Flash (LFA) technique is a fast, absolute, non-destructive, and non-contact method for accurate measurement of Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.thermal diffusivity. This innovative approach not only determines Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.thermal diffusivity, but also characterizes the specific heat of materials when a reference sample is used.

In the LFA process, the front surface of a plane-parallel sample is heated by a short pulse of energy. An infrared (IR) detector measures the resulting temperature change on the back of the sample. From these data, both Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.thermal diffusivity and specific heat can be characterized.

To calculate the Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity, these thermophysical properties are combined with the DensityThe mass density is defined as the ratio between mass and volume. density using the formula:

λ(T)=a(T)⋅cp​⋅ρ(T)

Where:

 

With its ability to analyze a wide range of materials at various temperatures, the LFA technique is essential for researchers and industries focused on understanding thermal properties in depth.

Cutaway view of a high-precision testing machine, featuring a red electromagnetic coil and blue light indicating operation.

Specifications

 LFA 717 HyperFlash®
Temperature Range-100°C to 500°C (RT version available)
Heating rate (max.)50 K/min
Measured thermal physical propertiesThermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.Thermal diffusivity and Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.specific heat capacity (and calculation of Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity)
Furnace cooling device
  • External chiller (RT to 500°C)

optional: 

  • Liquid nitrogen cooling (-100°C to 500°C)
  • Pressurized air (0°C to 500°C)
Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.Thermal diffusivity0.01 mm2/s to 2000 mm2/s
Thermal conductivity0.1 W/(m·K) to 4000 W/(m·K)
Xenon flash lamp
 
  • Pulse energy: up to 10 Joules/pulse (variable), software-controlled
  • Pulse width: 10 to 1500 μs
ZoomOptics Patented; optimized field of view (optional, requires no mask)
Pulse mappingFor finite pulse correction and improved cp determination
IR detectors
  • InSb: RT to 500°C
  • MCT: -100°C to 500°C
  • Detector refill device (option)
Vacuum< 150 mbar
Sample holders
  • Round and square specimen
  • Liquids, pastes, resins, powders, fibers, laminates, anisotropic materials
  • Tests under mechanical pressure
Customer support representative at a computer, smiling and engaged, highlighting NETZSCH's commitment to service excellence.


Proven Excellence in Service

At NETZSCH Analyzing & Testing, we offer a comprehensive range of services globally to ensure the optimal performance and longevity of your thermoanalytical equipment. With a track record of proven excellence, our services are designed to maximize the effectiveness of your devices, extend their lifespan, and minimize downtime. 

Unlock the full potential of your equipment with our tailored solutions, backed by years of industry expertise and innovation.

Software

Proteus® Software for LFA - Fast, efficient, and seamlessly integrated!

NETZSCH Assistant 9.5 interface displaying application options for Measurements, Analysis, Calibrations, and Service Tools.

The Proteus® 64-bit software is designed to be licensed with each instrument, allowing users to simultaneously connect multiple instruments via USB or run the software on secondary installations on different computer systems. Integrated into the NETZSCH Assistant starting with version 9.5, this software suite links a wide range of NETZSCH instruments and various third-party applications into a cohesive management platform.

A significant enhancement specific to Laser Flash Analysis (LFA) is the transition from the previous database format to a new, faster SQL database format. This upgrade in data architecture results in improved modeling times and can deliver results up to 2.5 times faster while using less memory. As a result, users can now store an almost unlimited number of measurements in a single database. All standard database management functions, including import/export and data merging, are still fully supported.

The LFA 717 HyperFlash® measurement software is an essential tool for connecting and controlling instrument and hardware accessories, allowing users to effectively define, monitor, and optimize measurements. Designed to enhance automation, this software offers a high degree of customization, making it ideal for various industries.

Dynamic Mechanical Analysis (DMA) 242 E Artemis measures properties of various materials, including human hair's response to shampoo.

In addition to measurement capabilities, the dedicated, stand alone Proteus® LFA  analysis software provides robust data analysis based on analytical models. Key features include:

Comprehensive data analysis:

Users can simultaneously analyze multiple measurements within a single plot, eliminating the need for post-processing. This streamlining saves time and improves accuracy.

Export detailed documentation:

Proteus® LFA provides extensive export options to generate comprehensive documentation of results, critical for quality assurance and reporting.

Save analysis states:

The ability to save analysis states allows convenient sequential analysis, making it easier to perform follow-up analyses without starting from scratch.

Graphs displaying thermal density measurements versus temperature, alongside detector signal data for analytical testing.

Unsurpassed integrated mathematical models for clear and precise evaluation. In addition to the standard model for opaque, homogeneous and isotropic samples, the so-called improved Cape-Lehman model, there are models for special application requirements and corrections.

Four software model illustrations for analyzing layers, translucency, permeability, and conductivity in material testing.

For better fit and best results, all models come standard with light pulse correction and baseline correction. The user has the option to turn off these corrections. All previously mentioned models take heat loss into account, in addition AdiabaticAdiabatic describes a system or measurement mode without any heat exchange with the surroundings. This mode can be realized using a calorimeter device according to the method of accelerating rate calorimetry (ARC). The main purpose of such a device is to study scenarios and thermal runaway reactions. A short description of the adiabatic mode is “no heat in – no heat out”.adiabatic (Parker) Model is also available.

Diagram illustrating heat loss, pulse measurement, and baseline correction in data analysis for engineering or scientific contexts.

In the latest version of our analysis software, we are pleased to introduce a refined and highly accurate pulse correction feature. This enhancement allows users to access samples that require exceptional time resolution, making it particularly beneficial for thin or highly conductive materials. It is especially useful when the light pulse overlaps with the thermal response of the sample.

Users can select from a variety of correction techniques within the calculation dialog:

  • Equivalent Square
  • Center of Gravity
  • Double Exponential Pulse Correction

 

Impact on Model Function and Fit Quality

Implementing pulse correction significantly affects both the appearance of the model function and the associated goodness of fit. For example, shown below is a high diffusivity material with a thermal diffusivity (α) of 800 mm²/s where a 1 ms pulse signal is superimposed on the detector signal.

The difference in calculated thermal diffusivity can exceed 20% depending on whether the exponential pulse correction is applied or not. This highlights the critical importance of using pulse correction techniques to achieve accurate analysis results.

Graphs and tables displaying data analysis results, including deviation percentage and goodness of fit metrics for experiments.
3D mass-loss curve and FT-IR spectra of gases released during DCP heating, showcasing absorbance and temperature variations.

This instrument is LabV®️-ready.

Turn data into better products with LabV®—a centralized, AI-driven material intelligence platform that integrates data from this instrument and any other data sources. Designed for R&D and QC engineers, LabV® enables data-driven decision-making to drive innovation and ensure consistently high-quality results.

E-Learning

Become an Expert with our Free E-Learning Courses

All NETZSCH E-Learning Basic Courses are free of charge! The content is created by our laboratory method experts, who share their personal experiences with you. Take advantage of flexible online learning, fully adapted to your training needs!

Please accept Marketing Cookies to see that Video.

A red Formula 1 car in the pit during a tire change, surrounded by focused team members in orange uniforms.

Consultancy & Sales

Do you have further questions about the instrument or the method and would like to speak to a sales representative?

Service & Support

Do you already have an instrument and need technical support or spare parts?

Downloads and Media

Please accept Marketing Cookies to see that Video.

The advanced design of the LFA 717 HyperFlash® offers enhanced temperature stability, fast measurement times, and non-contact infrared detection for accurate results. Intelligent software and versatile sample holders make it adaptable for various materials − from solids to liquids. Experience fast, precise, and versatile thermal analysis with our new system. 
AI Overview
An error occurred. Please try again.