19.06.2023 von Andrew Gillen, Aileen Sammler
Successful Installation of the First NETZSCH PicoTR in the Southern Hemisphere

The University of Wollongong, Australia (UOW) is one of the world's top modern universities, offering excellence in teaching, learning and research. It´s Institute for Superconducting and Electronic Materials (ISEM) is a world-class collaborative team conducting research in superconducting and electronic materials science and technology.
Distinguished Professor Xiaolin Wang heads the ISEM. His group has a keen interest in the world of extremes: Characterization of materials in ultra-thin film and ultra-high pressure environments. In June 2023, together with our colleagues from NETZSCH Japan, K.K. and NETZSCH Australia Pty Ltd, they installed the first PicoTR thermal analysis system in the southern hemisphere.
NanoTR and PicoTR are the thermal analysis systems of choice for thin films. They are the world’s first analyzers for providing high-precision measurements on thermophysical properties of metallic, oxide, organic and other films.

Pushing Boundaries: Revolutionary Research Unearths Unconventional Phenomena in Emerging Materials and Devices
In 2022, the University of Wollongong ISEM received funding to establish a unique Australian research facility: A combination of high-efficiency thin film thermophysical property analyzer and a complete package of tools for materials and devices fabrication and characterization at ultra-high pressures.
This exceptionally comprehensive and versatile set of tools will foster collaborative activities in Australia and worldwide supporting breakthrough research to discover novel unconventional phenomena in topological insulators, superconductors, spintronic materials, low energy devices, one- and two-dimensional micro- and nanomaterials, battery and biomagnetic materials.
The functionality of many materials critically depends on their capability of operating under extreme conditions, for many applications in energy generation, barocaloric cooling and structural materials in fusion or space technology. Currently, there is a great focus on emerging ultra-thin and 2D forms of materials derived from van-der Waals compounds.
NETZSCH is happy to be part of these groundbreaking research activities: Thus, on June 9, 2023, the PicoTR system with X-Y stage and temperature control system (-100 - 500°C) was successfully installed at University of Wollongong’s ISEM by NETZSCH.
Originally developed by the National Institute of Advanced Industrial Science and Technology (AIST), Japan, the NETZSCH PicoTR thermophysical property analyzer is a unique instrument specifically designed to measure thermal conductivity, thermal diffusivity, thermal effusively, and interlayer thermal resistance of thin films in the range 10nm…1µm.
Applications include:
- Thermoelectric material, solar cell, fuel cell, OLED.
- Semiconductor memory, storage, metals, FeRAM, MRAM, PRAM, LSI, power devices, phase change and magnetic recording film, diffusion barrier film.
- LED, ceramic composites, electronics, resins for insulation films, transparent conductive films for FPD, interlayer dielectrics, gate insulators.

PicoTR’s state-of-the-art signal processing technology allows for high speed measurements. With this ThermoreflectanceThermoreflectance ist eine Methode zur Bestimmung der Temperaturleitfähigkeit und Wärmeleitfähigkeit von Proben mit Dicken im Nano- und Mikrometer-Bereich.thermoreflectance apparatus, a laser pulse of 0.5-ps pulse width is periodically irradiated to the sample. The resulting temperature response is applied to a pulse laser (probe laser). Excellent s/n ratio can be attained by high-speed integration of repetitive signals. It can be easily switched between the RF and FF configurations though the software for a wide variety of samples.
Learn more about the NETZSCH PicoTR here.
Learn more about University of Wollongong’s ISEM here.
More Blog Articles about PicoTR
- 07.10.2026
From the Green Body to a Dense Ceramic – How NETZSCH Termica Neo Makes Sintering Transparent

- 03.10.2026
Was die DSC über die Alterung von Polypropylen verrät

- 22.09.2026
Analysegeräte von NETZSCH im Einsatz bei führenden Forschungseinrichtungen Südkoreas

- 09.09.2026
Einführung in die Rheologie von Dispersionen – Grundlagen, Einflussfaktoren und Messmethoden

- 04.08.2026
Künstlicher Knorpel auf dem Prüfstand: Rheologie liefert entscheidende Erkenntnisse

- 23.07.2026
Mehr als nur Hitze und Rauch: Die Bedeutung der Gasanalyse bei modernen Brandversuchen

- 23.07.2026
Rheodialysis: Controlling Chemistry and Shear Simultaneously with the NETZSCH Kinexus Rheometer

- 13.07.2026
Thermoplastic Crystallization – Understanding PA12 During Cooling