28.04.2021 by Milena Riedl, Dr. Natalie Rudolph

Material Science in Additive Manufacturing: Which Materials are Commonly Used?

A gloved hand gestures towards molecular structures, highlighting common materials used in additive manufacturing technology.

Before we dive into the material science of processing materials with different Additive Manufacturing technologies, we introduce common material groups, distinct molecular structures of material classes as well as discuss other materials used for non-technical applications.

In the basic section of our “Material Science in Additive Manufacturing” video series, the focus was on understanding the different Additive Manufacturing (AM) technologies, process principles, materials, benefits and advantages, including where the different technologies and processes are applied in industry today.

In the advanced section, we will dive deeper and look at the underlying material science as well as the methods suitable to analyze the materials and to optimize processes.

This week’s topic: Overview of Materials Used in Additive Manufacturing

  • Introduction to the common material groups: Thermoplastics, thermosets and metals
  • Different molecular structure of material classes
  • Other materials in AM used for non-technical applications of industrial 3D printing

Please accept Marketing Cookies to see that Video.

Description

More Additive Manufacturing content by NETZSCH

We took questions related to common 3D printing issues and categorized them into what we call 3D printing myths – common concerns and sometimes misconceptions of this industry.

The videos are available here!

Green 3D-printed object displayed under a printer, showcasing advances in polymer additive manufacturing techniques.

FREE E-Book

Thermal Analysis and Rheology in Polymer Additive Manufacturing

Discover the secrets behind AM's game-changing capabilities! Our newly released ebook delves deep into the heart of AM, unveiling the power of reliable material characterization techniques, specifically thermal analysis and rheology.

AI Overview
An error occurred. Please try again.