Colorful oil slick on water surface, showcasing iridescent patterns and textures, highlighting environmental contamination.

11.03.2025 by Aileen Sammler

Understanding the Role of Tar Materials in Anode Production by Means of NETZSCH Analysis Instruments

Tar plays a key role in the production of high-performance battery grade graphite anode materials. During PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis at elevated temperatures, tar carbonizes and helps form the anode particles. The softening point of the tar determines the temperature range at which the material will sufficiently liquefy to ensure homogeneous distribution in the composite. 

The Importance of Tar in Graphite Anode Manufacturing

Tar plays a key role in the production of high-performance battery grade graphite anode materials. During PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis at elevated temperatures, tar carbonizes and helps form the anode particles. The softening point of the tar determines the temperature range at which the material will sufficiently liquefy to ensure homogeneous distribution in the composite. A higher softening point results in a more uniform coating, which is critical for anode performance. After thermal treatment, the carbonaceous residue remains structurally stable and retains its essential thermal and chemical resistance, a key factor in high-temperature applications.

NETZSCH’s Thermal Analysis methods such as Thermogravimetry (TG or thermogravimetric analysis, TGA) and Differential Scanning Calorimetry (DSC) can be used to assess the suitability of different tar types for anode production.

Experimental Approach: Thermal Analysis of Tar Materials

Four different types of tar were analyzed using the NETZSCH TG 309 Libra® for thermogravimetric measurements and the NETZSCH DSC 300 Caliris® for Phase TransitionsThe term phase transition (or phase change) is most commonly used to describe transitions between the solid, liquid and gaseous states.phase transition and softening point determination. The TGA experiments were performed under inert conditions up to 900°C and then in an oxidative atmosphere up to 1100°C. DSC measurements were performed to evaluate the Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.glass transition temperatures and other caloric effects of the tar samples.

Key Findings from the Analysis

2. Differential Scanning Calorimetry (DSC):

Green 3D-printed object being produced in a professional additive manufacturing setup, showcasing advanced polymer technology.
The NETZSCH DSC 300 Caliris®

Implications for Anode Material Selection

The combination of TGA and DSC analysis provides a comprehensive evaluation of tar materials, allowing manufacturers to determine their Thermal StabilityA material is thermally stable if it does not decompose under the influence of temperature. One way to determine the thermal stability of a substance is to use a TGA (thermogravimetric analyzer). thermal stability, carbon yield, and Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.glass transition behavior. This information is essential for selecting the most appropriate raw materials, optimizing formulations, and ensuring consistency in anode production. By carefully evaluating tar properties, manufacturers can improve battery efficiency and longevity, leading to improved performance in high-temperature applications.

Watch also our webinar “Introduction to Battery Testing by Thermal Analysis”: 

Please accept Marketing Cookies to see that Video.

Learn more about the NETZSCH DSC 300 Caliris® and TG 309 Libra®

  • DSC 300 Caliris® Classic

    Quality assurance of polymers, food, cosmetics and organics

    • Compact design for more space in the lab
    • Temperature range: -170°C to 600°C
    • Automatic Sample Changer: Up to 20 samples and references
  • DSC 300 Caliris® Select

    Quality assurance of polymers, food, cosmetics and organics

    • Choose your appropriate module: Standard, Polymer or High-Performance
    • Temperature range: -180°C to 750°C
    • Automatic Sample Changer: Up to 192 + 12 samples and references
  • DSC 300 Caliris® Supreme

    Quality assurance of polymers, food, cosmetics and organics

    • Three easily interchangeable modules: Standard, Polymer and High-Performance
    • Temperature range: -180°C to 750°C
    • UV-Accessory: Investigate curing reactions with photo-calorimeter
  • TG 309 Libra® Classic

    Ensure product quality by detecting mass changes with the perfect thermobalance for quality control!

    • Balance Resolution: 50ng
    • Temperature range: RT (10°C) to 1025°C at the sample
    • Automatic Sample Changer: 20 sample and reference spaces
  • TG 309 Libra® Select

    Our work horse for testing in laboratories, including industrial development labs!

    • Balance Resolution: 20ng
    • Temperature range: RT (10°C) to 1025°C/1100°C at the sample
    • Automatic Sample Changer: 204 sample and reference spaces
  • TG 309 Libra® Supreme

    Ensure product quality and safety with the all-in-one instrument for research labs in academia and industry!

    • Balance Resolution: 10ng
    • Temperature range: RT (10°C) to 1100°C at the sample
    • Automatic Sample Changer: 204 sample and reference spaces
Graph illustrating dynamic mechanical analysis, showing E' and E'' values for oil, melt, polymer, and metal with angle δ.

Total Battery Energy Solutions by NETZSCH

The NETZSCH Group provides total solutions for battery applications, from grinding and dispersing of battery materials, stable and contamination free pumping to stability, charging and discharging efficiency and even recycling. 

Visit www.energy.NETZSCH.com to learn more.

AI Overview
An error occurred. Please try again.