Delamination (Time to Delamination)

Delamination refers to the separation of layers from one another – e.g., of a resin from a laminate or of fibers from a resin. Such processes cause defects in printed circuit boards. 

ICP-TM-650 No. 2.4.24.1 describes the method of determining the time to delamination for laminates and printed boards through the use of a thermomechanical analyzer (TMA).

The sample is heated to a specified IsothermalTests at controlled and constant temperature are called isothermal.isothermal temperature at 10 K/min and is then held at this temperature for 10 minutes or until failure (see figure 1).

Scan graph depicting epoxy material behavior at 260°C showing dimensional thickness and temperature changes over time.
Figure 1: Typical scan of an epoxy material at 260°C (taken from ICP-TM-650 No. 2.4.24.1)