TGA-FT-IR Transfer Line Coupling: High Interface Temperature and Minimal Maintenance Effort

Thermal stability and evolved gas analysis of high-boiling materials are essential in various application fields. The evaporation of glycerol from cosmetic formulations, volatilizing of plasticizers from polymers and the analysis of petrochemical fragments are only a few examples, where high-interface temperature between the outlet of the thermobalance and the inlet of the FTIR gas cell is absolutely required.

DSC 300 Caliris® by NETZSCH showcases advanced design and modular capabilities for differential scanning calorimetry. Celebrating 60 years of innovation.
Coupling sceme: completely heated interface from TG outlet to FTIR gas cell

Please accept Marketing Cookies to see that Video.

Bruker & NETZSCH: Evolved Gas Analysis Coupled to Thermal Analysis by Means of Infrared Spectroscopy

Together, NETZSCH and Bruker Optics developed the perfect solution with the ability to heat all interface materials, such as the coupling adapter and transfer line, up to 400°C.

Even the gas cell can be heated up to 370°C. These high temperatures enable loss-free transfer of high-boiling materials without tailing or condensation. Chemical or mechanical cleaning of the tubing is not necessary.

In case of trace amounts of impurities in the gas cell despite heating to 370°C, an automatic heat cleaning procedure is included in the heating control. The user may set the temperature of the gas cell to 400°C, then the automatic cleaning procedure starts, which means heating the gas cell to 400°C for 35 minutes and then automatically cooling back to 370°C in preparation to the next measurement. The residuals in the gas cell are vaporized and purged out immediately.

Bruker gas cell display showing temperature settings of 370°C and 400°C for evolved gas analysis, highlighting advanced thermal stability.

The high interface temperature together with this automatic cleaning procedure ensure a long lifetime and no need for purification of all coupling parts, e.g., tubing and FT-IR gas cell windows.

See here a dedicated application example for the investigation of high-boiling organics:

Learn more about NETZSCH instruments and coupling solutions:

Subscribe to our newsletter

Get exclusive insights into brand new applications & trends in thermal analysis.

Subscribe now
AI Overview
An error occurred. Please try again.