13.07.2026 by Aileen Sammler
Thermoplastic Crystallization – Understanding PA12 During Cooling

This is blog 4 of the series: “The New Dimension of Thermal Analysis with NETZSCH Termica Neo: The Software for Thermal Simulation of Chemical Reactions on an Industrial Scale.”
Read about the following topics in this series: Understanding PA12 During Cooling
Cooling decides everything.
The moment PA12 (polyamide 12) transitions from a molten to a solid state, its internal structure forms: crystal by crystal and layer by layer. Small changes in the cooling rate can result in significant differences in Crystallinity / Degree of CrystallinityCrystallinity refers to the degree of structural order of a solid. In a crystal, the arrangement of atoms or molecules is consistent and repetitive. Many materials such as glass ceramics and some polymers can be prepared in such a way as to produce a mixture of crystalline and amorphous regions.crystallinity, shrinkage, strength, and dimensional stability.
With NETZSCH Termica Neo, you can see that transition as it happens: a moving CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.crystallization front, heat release, and the shifting thermal field inside the material.

Why CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.Crystallization Needs Spatial Understanding
CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.Crystallization isn’t a uniform event. As PA12 cools:
- The surface solidifies first.
- The core stays warm for longer.
- An ExothermicA sample transition or a reaction is exothermic if heat is generated.exothermic CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.crystallization wave travels through the thickness.
- Final morphology depends on how quickly each region passes through the CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.crystallization window.
DSC curves only show the bulk CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.crystallization peak, not where or when structure forms inside the real part.
Termica Neo closes that gap.
How Termica Neo Simulates PA12 CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.Crystallization
The NETZSCH software imports CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released. crystallization kinetics from Kinetics Neo and applies them to real-world geometry and thermal boundary conditions.
You define:
- cooling environment (air, mold, insulated)
- geometry (plate, cylinder, sphere, rotational body)
- initial melt temperature
- heat transfer coefficients and emissivity
Termica Neo calculates:
- temperature distribution during cooling
- local CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released. crystallization onset and rate
- movement of the CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released. crystallization front
- heat release from CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released. crystallization impacting nearby regions
The result is a full, spatially resolved view of polymer solidification.
The PA12 Case: What the Simulation Reveals
In the brochure’s PA12 example, Termica Neo simulates a long cylinder bar cooling from melt temperature down to 50°C. The results show:
- A CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released. crystallization band forms between approx. 150–170°C.
- This band moves inwards, creating a visible reaction front.
- Faster cooling shifts crystallization to lower temperatures.
- Slower cooling yields a more uniform morphology but longer cycle times.
What you see is a dynamic transformation: thermal gradients driving structural gradients.
To learn more take a look at the brochure:
Why This Matters for the Process and the Product
Cooling is often the least controlled part of polymer processing, yet it determines:
- warpage and shrinkage
- mechanical consistency
- dimensional accuracy
- cycle time
- surface quality
Termica Neo lets you experiment virtually with cooling rates, tooling materials, and temperature programs until the internal structure of the part is exactly as you want it. No guesswork, no surprises. Just predictable solidification.

Benefits of Termica Neo
- Imports crystallization kinetics from Kinetics Neo
- Realistic simulation of cooling and crystallization coupling
- 2D/3D visualization of temperature, crystallization rate, and degree of conversion
- Optimization of cooling strategies and morphology control
- Shorter development cycles | Fewer trials | Higher consistency
About This Blog Series
This article continues the NETZSCH series: “The New Dimension of Thermal Analysis with Termica Neo: Software for the Thermal Simulation of Chemical Reactions on an Industrial Scale.”
Already published articles: (see links below)
- From Kinetic Model to Real-World Application — turning 1-D data into 3-D insight.
- Scale-up & Safety — predicting runaways before they happen.
- Polymer Curing — How Termica Neo Makes Curing Visible
- Thermoplastic Crystallization– Understanding PA12 During Cooling
Stay tuned for our last article of this series: We will talk about ceramic SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering – from the green body to a DensityThe mass density is defined as the ratio between mass and volume. density gradient with NETZSCH Termica NEO.
--------------------------
Useful Links:
Get your free demo version:Request Demo Version of Temica Form - NETZSCH Termica Neo
Download the new brochure to learn more:Termica Neo Brochure
Direct contact:Feature Request - NETZSCH Kinetics Neo
Learn even more:Termica Neo - NETZSCH Termica Neo
This webinar could be of interest to you:
These blog articles may also be of interest
- 07.10.2026
From the Green Body to a Dense Ceramic – How NETZSCH Termica Neo Makes Sintering Transparent

- 13.07.2026
Thermoplastic Crystallization – Understanding PA12 During Cooling

- 14.05.2026
Polymer Curing – How NETZSCH Termica Neo Makes Curing Visible

- 03.03.2026
Scale-Up & Safety: How NETZSCH Termica Neo Predicts What Could Go Wrong

- 03.02.2026
From Kinetic Model to Real-World Application: How NETZSCH Termica Neo Simulates Thermal Reactions

- 06.05.2024
NETZSCH Tech Talk – Spring Edition:Unveiling Thermal Innovations in Just 30 Minutes

- 07.02.2024
Introducing Termica Neo: The New NETZSCH Software for Thermal Simulation in Industrial Settings