Analyzing & Testing
Blog
Career
Contact
English
English
German
English (Australia)
English (USA)
Spanish
French
Italian
Japanese
Korean
Polish
Portuguese (Brazil)
Greek
Turkish
Arabic
Russian
Indonesian
Danish
Bulgarian
Romanian
Hungarian
Dutch
Czech
Swedish
Finnish
NETZSCH Group
Proven Excellence in mechanical engineering for over 150 years
Analyzing & Testing
NETZSCH devices for thermal analysis, rheology as well as fire testing devices
Pumps & Systems
Innovative customised solutions in handling complex media
Grinding & Dispersing
Extensive range of machines for grinding and dispersing
Blog
Career
Contact
Ask the AI
Products
Products
Thermal Analysis / Calorimetry
Differential Scanning Calorimeter (DSC/DTA)
Simultaneous Thermal Analyzer (STA/TGA-DSC)
Thermogravimetric Analyzer (TGA)
Thermomechanical Analyzer (TMA)
Dynamic Mechanical Analyzer (DMA)
Multiple Module Calorimeter (MMC)
Dilatometer (DIL)
Accelerating Rate Calorimeter (
ARC
®
)
Dielectric Analyzer (DEA)
Refractory Tester
Thermophysical Properties Analysis
Light/Laser Flash Analyzer (LFA)
Time Domain Thermoreflectance Analyzer (TDTR)
Heat Flow Meter (HFM) / Guarded Heat Flow Meter (GHFM)
Guarded Hot Plate/Pipe (GHP/TLR)
Hotbox Test Chambers
Evolved Gas Analysis
Evolved Gas Analysis Overview (EGA)
Fourier Transform Infrared Spectroscopy (FT-IR)
Mass Spectrometry (MS)
Gas Chromatography-Mass Spectrometry (GC-MS)
Rheology
Rotational Rheometers
Capillary Rheometers
Fire Testing
Fire Testing Systems for the Automotive Industry
Fire Testing Systems for the building industry
Fire Testing Systems for Cables
Fire Testing Systems for Electronics and Polymers
Fire Testing Systems for Smoke Density Analysis
Special Constructions of Fire Testing Systems
Software
Software
Applications
Applications
Customer Success Stories
Polymers
Adhesives & Sealants
Batteries
Biomass
Building Materials
Ceramics & Glass
Inorganics
Metals & Alloys
Nuclear
Organics
Life Sciences
Photovoltaics
Thermal Insulation
Thermoelectric
Know-How
Know-How
NETZSCH Online Academy
Customer Success Stories
Glossary
Blog
Tips & Tricks
Application Notes
White Papers
Application Books
Poster
Software Innovations
Materials Insights
Services
Services
Proven Excellence in Service
How to Get in Contact with Us
Hotline and Remote Support
Repair Service
FAQ Service
Consumables, Spare-Parts, Accessories
Service-Level Agreement
Service in Regulated Areas
Unlimited Warranty by NETZSCH
Training & Seminars
Contract Testing
Newsletter Service
Glossary
E-Learning
E-Learning
(DSC) Differential Scanning Calorimetry Courses
(STA/TGA-DSC) Simultaneous Thermal Analysis Courses
(TG) Thermogravimetry Courses
(DMA) Dynamic Mechanical Analysis Courses
(DIL) Dilatometry Courses
(LFA) Light/Laser Flash Analysis Courses
(HFM) Heat Flow Meter Courses
Rheology Courses
Events
Events
Tradeshows
Seminars
Webinars
Conferences
Ask the AI
Open/close navigation
Analyzing & Testing
Services
Products
Products
Thermal Analysis / Calorimetry
Differential Scanning Calorimeter (DSC/DTA)
Simultaneous Thermal Analyzer (STA/TGA-DSC)
Thermogravimetric Analyzer (TGA)
Thermomechanical Analyzer (TMA)
Dynamic Mechanical Analyzer (DMA)
Multiple Module Calorimeter (MMC)
Dilatometer (DIL)
Accelerating Rate Calorimeter (
ARC
®
)
Dielectric Analyzer (DEA)
Refractory Tester
Thermophysical Properties Analysis
Light/Laser Flash Analyzer (LFA)
Time Domain Thermoreflectance Analyzer (TDTR)
Heat Flow Meter (HFM) / Guarded Heat Flow Meter (GHFM)
Guarded Hot Plate/Pipe (GHP/TLR)
Hotbox Test Chambers
Evolved Gas Analysis
Evolved Gas Analysis Overview (EGA)
Fourier Transform Infrared Spectroscopy (FT-IR)
Mass Spectrometry (MS)
Gas Chromatography-Mass Spectrometry (GC-MS)
Rheology
Rotational Rheometers
Capillary Rheometers
Fire Testing
Fire Testing Systems for the Automotive Industry
Fire Testing Systems for the building industry
Fire Testing Systems for Cables
Fire Testing Systems for Electronics and Polymers
Fire Testing Systems for Smoke Density Analysis
Special Constructions of Fire Testing Systems
Software
Software
Applications
Applications
Customer Success Stories
Polymers
Adhesives & Sealants
Batteries
Biomass
Building Materials
Ceramics & Glass
Inorganics
Metals & Alloys
Nuclear
Organics
Life Sciences
Photovoltaics
Thermal Insulation
Thermoelectric
Know-How
Know-How
NETZSCH Online Academy
Customer Success Stories
Glossary
Blog
Tips & Tricks
Application Notes
White Papers
Application Books
Poster
Software Innovations
Materials Insights
E-Learning
E-Learning
(DSC) Differential Scanning Calorimetry Courses
(STA/TGA-DSC) Simultaneous Thermal Analysis Courses
(TG) Thermogravimetry Courses
(DMA) Dynamic Mechanical Analysis Courses
(DIL) Dilatometry Courses
(LFA) Light/Laser Flash Analysis Courses
(HFM) Heat Flow Meter Courses
Rheology Courses
Events
Events
Tradeshows
Seminars
Webinars
Conferences
Services
Proven Excellence in Service
How to Get in Contact with Us
Hotline and Remote Support
Repair Service
FAQ Service
Consumables, Spare-Parts, Accessories
Service-Level Agreement
Service in Regulated Areas
Unlimited Warranty by NETZSCH
Training & Seminars
Contract Testing
Newsletter Service
Glossary
Kicker
Commodity Thermoplastics
Lead
Insert Text
Lead
Insert Text
CTP
Commodity Thermoplastics
ABS
CTP
Acrylonitrile-Butadiene-Styrene Copolymer
Glass Transition Temperature
-85/95 to 105/(125)°C
Melting Temperature
-
Specific Heat Capacity
1.26 to 1.68 J/(g*K)
ASA
CTP
Acrylonitrile-Styrene-Acrylate Copolymer
Glass Transition Temperature
50 to -40°C / 95 to 105°C
Melting Temperature
-
Specific Heat Capacity
1.3 to 1.4 J/(g*K)
EVA
CTP
Ethylene Vinyl Acetate
Glass Transition Temperature
-40 to +20°C
Melting Temperature
30 to 110°C
Specific Heat Capacity
2.3 J/(g*K)
PB
CTP
Polybutene
Glass Transition Temperature
-30 to +20°C
Melting Temperature
115 to 135°C
Specific Heat Capacity
1.8 to 2.0 J/(g*K)
PE-HD
CTP
Polyethylene High Density
Glass Transition Temperature
-130 to -100°C
Melting Temperature
125 to 135°C
Specific Heat Capacity
1.8 to 2.7 J/(g*K)
PE-LD
CTP
Polyethylene Low Density
Glass Transition Temperature
-130 to -100/-30 to -10°C
Melting Temperature
100 to 115°C
Specific Heat Capacity
1.8 to 3.4 J/(g*K)
PE-LLD
CTP
Polyethylene Linear Low Density
Glass Transition Temperature
-130 to -100/-70 to -25°C
Melting Temperature
122 to 127°C
Specific Heat Capacity
-
PE-UHMW
CTP
Polyethylene Ultra High Molecular Weight
Glass Transition Temperature
-130 to -100°C
Melting Temperature
130 to 145°C
Specific Heat Capacity
1.84 J/(g*K)
PIB
CTP
Polyisobutylene
Glass Transition Temperature
-70 to -60°C
Melting Temperature
-
Specific Heat Capacity
1.97 J/(g*K)
PLA
CTP
Polylactide (Polylactic Acid)
Glass Transition Temperature
45 to 65°C
Melting Temperature
150 to 160°C
Specific Heat Capacity
-
PP (isotactic)
CTP
Polypropylene
Glass Transition Temperature
-20 to 20°C
Melting Temperature
160 to 165°C
Specific Heat Capacity
1.8 J/(g*K)
PS
CTP
Polystyrene
Glass Transition Temperature
80 to 105°C
Melting Temperature
-
Specific Heat Capacity
1.3 J/(g*K)
PVAL
CTP
Polyvinyl Alcohol
Glass Transition Temperature
70 to 100°C
Melting Temperature
220 to 260°C
Specific Heat Capacity
1.55 J/(g*K)
PVC-P
CTP
Polyvinylchloride (with plasticizer)
Glass Transition Temperature
-50 to 80°C
Melting Temperature
-
Specific Heat Capacity
0.8 to 0.9J/(g*K)
PVC-U
CTP
Polyvinyl Chloride (Unplasticized)
Glass Transition Temperature
80 to 90°C
Melting Temperature
-
Specific Heat Capacity
0.84 to 1.17 J/(g*K)
SAN
CTP
Styrene-Acrylonitrile Copolymer
Glass Transition Temperature
95 to 110/(125)°C
Melting Temperature
-
Specific Heat Capacity
1.18 to 1.20 J/(g*K)
SB
CTP
Styrene/Polybutadiene copolymer
Glass Transition Temperature
-90 to -50 / 80 to 110°C
Melting Temperature
-
Specific Heat Capacity
1.2 to 1.3 J/(g*K)