General Properties
Short Name: UP
Name: Unsaturated Polyester Resin
Unsaturated polyester resins (UP) are reaction resins with double bonds in the macromolecular backbone. These are a pre-requisite for copolymerization reactions without separation of reaction products. It is therefore possible to employ aluminum crucibles with pierced lids for their DSC investigation – just like for epoxy resins. Unsaturated polyester resins are available as cast resins, molding compounds or prepregs.
Structural Formula

Properties
NETZSCH Measurement

| Sample Mass | 15.63 mg |
| Heating Rates | 20 K/min |
| Crucible | Al, pierced lid |
| Atmosphere | N2 (40 ml/min) |
Evaluation
The DSC curve shown above indicates a Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.glass transition (midpoint 66°C) in the 1st heating, followed by two small overlapping peaks (attributable to the melting of additives) and post-Curing (Crosslinking Reactions)Literally translated, the term “crosslinking“ means “cross networking”. In the chemical context, it is used for reactions in which molecules are linked together by introducing covalent bonds and forming three-dimensional networks.curing with a peak temperature of 191°C and a reaction enthalpy of approx. 4 J/g.