The Fleshed-Out Design of the QMS 505 Aëolos® for Coupling to TGA, STA, DSC and DIL Systems
The 505 Aëolos® Quadro quadrupole mass spectrometer is a new compact mass spectrometer with a heated capillary inlet system for routine analysis of gases and, in particular, volatile Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition products of thermal analysis. This system is optimized for coupling to differential scanning calorimeters (DSCs), thermogravimetric analyzers (TGAs) and dilatometers (DILs). The software is unique: fully integrated MS software for measurement and analysis.

Capillary Coupling for Optimized Gas Flow Conditions
- Single-step pressure reduction
- Minimization of cold spots in the entire transfer path of the gases due to an even temperature of up to 400°C (adaptor 400°C, transfer line up to 350°C)
- Heated chamber for easy handling and precise adjustment of the quartz glass capillary inlet to the QMS
- Flexible, allowing standard thermoanalytical measurements and also simultaneous TGA-DSC-MS-GC-MS and TGA-DSC-MS-FT-IR measurements
- Very robust and service-friendly while still maintaining high sensitivity (detectable mass loss in the μg-range)
- TGA-MS measurements under humid atmospheres possible
- Hyperbolic quadrupole system with pre-filter for improved transmission in the high mass range and improved sensitivity in the low mass range (e.g., H2, He)
- SEM with discrete dynodes and integrated Faraday cup for high dynamic range and long lifetime
- 3-D presentation of MS and thermal analysis data
- Operation and data evaluation with Proteus® software
Sophisticated Heated Transfer System and Single-Step Pressure Reduction for Loss-Free Gas Transport
The high temperature of the gas transfer system and the absence of pressure reduction orifices practically eliminate condensation of Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition products during thermal analysis experiments. This achieves a high detection sensitivity and facilitates quantitative detection of all identified gas components.
The inlet system with the capillary allows for the investigation of other gas sources independent of the thermoanalytical system.
Design of the NETZSCH Thermal Analyzers
Already from the outset, NETZSCH thermal analysis devices were developed with the possibility of coupling in mind. Over the last 40 years, the gas transport path – which starts at the furnace outlet and progresses via the adapter and capillary up to the QMS inlet – has been considered and optimized at every new phase in development. Today, any gas loss caused by condensation at cold spots has nearly been eliminated; also, very low carrier gas flow rates are sufficient for complete transfer. The minimal dilution of the volatile sample products released results in high detection sensitivity with the TGA/STA/DIL-QMS 505 Aëolos®.

Application Areas of the QMS 505 Aëolos® Coupling
- Dehydration
- Stability
- Residual Solvent
- PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.Pyrolysis
- Combustion
- OxidationOxidation can describe different processes in the context of thermal analysis.Oxidation
- Corrosion
- Adsorption
- Desorption
- Catalysis
Composition Analysis
- Polymer Content
- Proximate Analysis
- Binder Burn-Out
- Dewaxing
- Ash ContentThe ash is a measure of the mineral oxide content on a weight basis. Thermogravimetric analysis (TGA) in an oxidative atmosphere is a well-proven method to determine the inorganic residue, commonly referred to ash, in organic materials such as polymers, rubbers, etc. Therefore, the TGA measurement will identify if a material is filled and calculates the total filler content.Ash Content
Evaporation
- Vapor Pressure
- Sublimation
The future is now!
Bring our devices into your laboratory with the click of a button.
Simply scan the QR code and get a 3D model of the instrument directly on your mobile phone or tablet. With the help of the latest AR Technology (Artificial Reality), the 3D model can easily be placed in your laboratory in its original life size. This function is browser-based and requires no app.
Find out and be amazed!

Request a Quote
Technical Data
Vacuum system
Adjustable interface temperature
Cathodes/Filaments

Mass range:
1 u to 300 u, optionally 512 u, including autotuning
Ion source:
Cross beam El
Detector:
SEM with discrete dynodes and integrated Faraday cup
Capillary:
Quartz-glass (max. 300°C), optionally stainless steel (max. 350°C), with supply coil, easily exchangable
Pressure reduction:
Single-step, from 10³ mbar to 5x10-6 mbar, no orifice
QMS measuring modes:
Scan analog, scan bargraph, MID
Application Literature