This product was removed from our portfolio.

Highlights

Method and Technique for the Characterization of Thermoelectric Materials

The Electrical Conductivity (SBA)Electrical conductivity is a physical property indicating a material's ability to allow the transport of an electric charge.SBA 458 Nemesis® offers a versatile measurement setup that accommodates a wider range of sample geometries than is typically possible with this technique. This system enables measurements of Electrical Conductivity (SBA)Electrical conductivity is a physical property indicating a material's ability to allow the transport of an electric charge.electrical conductivity—a physical property indicating a material's ability to transport electric charge—at temperatures up to 1100°C.

One of the standout features of the Electrical Conductivity (SBA)Electrical conductivity is a physical property indicating a material's ability to allow the transport of an electric charge.SBA 458 Nemesis® is its quick and convenient sample change process. Samples can be swapped out swiftly and effortlessly by hand, without the need for any tools. The use of sheathed thermocouples in the setup prevents the samples from sticking to the electrodes, ensuring smooth transitions between measurements.

The system also integrates a quality check mechanism through its innovative two-heater design. These heaters operate alternately at each temperature step, allowing for the immediate detection of deviations from linearity or hysteresis, which could indicate inaccurate measurements. This proactive monitoring enhances the reliability of the results.

Additionally, the fixed positions of the thermocouples mean that the often cumbersome process of determining their distance before each measurement is no longer necessary. This removal of a potential error source significantly enhances the precision and reproducibility of Electrical Conductivity (SBA)Electrical conductivity is a physical property indicating a material's ability to allow the transport of an electric charge.electrical conductivity measurements.

Red safety cap labeled "Remove before closing furnace" on laboratory equipment with metallic base, indicating proper handling protocols.

The unique design of the Electrical Conductivity (SBA)Electrical conductivity is a physical property indicating a material's ability to allow the transport of an electric charge.SBA 458 Nemesis® allows for a quality check of both the Seebeck coefficient and Electrical Conductivity (SBA)Electrical conductivity is a physical property indicating a material's ability to allow the transport of an electric charge.electrical conductivity. Even before a time-consuming temperature program is started, this quality check indicates whether a measurement can be performed without any errors. In addition, the quality check is performed at each temperature step, monitoring the correctness of the measurement results for the Seebeck coefficient and the Electrical Conductivity (SBA)Electrical conductivity is a physical property indicating a material's ability to allow the transport of an electric charge.electrical conductivity

The SBA 458 Nemesis® is a truly new method for determination of the Seebeck coefficient (S) and Electrical Conductivity (SBA)Electrical conductivity is a physical property indicating a material's ability to allow the transport of an electric charge.electrical conductivity (σ). Its novel setup and clever, practical design offer numerous unparalleled advantages. Perhaps the most significant of these is elimination of the disadvantages inherent in conventional methods – thus allowing for the reliable and precise determination of the two thermophysical properties S and σ.

Using current pins and thermocouples on the sample’s lower surface, the electrical conductivity is determined by the 4-point method. Micro heaters are placed below the two sample edges, creating temperature gradients in both sample directions. The resulting voltage is measured by the thermocouple wires and then used for calculation of the Seebeck coefficient.

Using the SBA 458 Nemesis® along with our Laser/Light Flash Analyzer, Differential Scanning Calorimeter and Dilatometer systems, it is now possible to determine a complete set of thermophysical properties directly related to the efficiency of thermoelectric materials, including:

Shear viscosity versus shear rate graph comparing two similar rubber samples, highlighting their indistinguishable flow behavior.
Graph showing the linear relationship between voltage and current, confirming the quality of the Seebeck coefficient.
Plot A: Quality check of the Seebeck coefficient is confirmed by the linear behavior of the voltages.

Seebeck Coefficient

A temperature gradient is generated in both sample directions by two micro heaters operating in alternation. While the cyclic heating is in progress, the resulting voltages (UA, UB) are measured. UA and UB are the voltages between the two positive and two negative thermocouple wires which are plotted against the temperature difference (ΔT; for both directions). ΔT is determined by two thermocouples (plot A).

The resulting large number of measuring points is the basis for calculation of a regression line. From the slope of the regression line, the Seebeck coefficient can be precisely determined:

  • All measurement points lie on a straight line → well-performed measurement (see plot A)
  • Deviation of the measurement points from the straight line, e.g., hysteresis → poor measurement

Electrical Conductivity

At each testing temperature, different current values will be applied to the sample several times by current pins. These values will be applied in both sample directions and the resulting voltages (UA, UB) will be measured (plot B). 

This process yields a large number of measurement points, allowing for a quality check prior to and during the measurement of all temperature steps:

  • All measurement points lie on a straight line and the two curves are superimposed → well-performed measurement (see plot B)
  • Deviation of the measurement points from the straight line or the two curves are not congruent with each other → poor measurement
Kinetics Neo logo, combining colorful geometric shapes, symbolizes advanced predictive modeling for UV-cured resin systems in material research.
Plot B: Quality check of the electrical conductivity is confirmed by the linear behavior of the measurement points.

Specifications

 SBA 458 Nemesis®
DesignTwo-heater system, quality check, horizontal sample arrangement
Temperature ranges of the exchangeable furnaces
  • -125°C ... 500°C
  • RT ... 1100°C
Temperature setting rangeUnlimited number of temperature steps
Thermocouples
  • Inconel®-sheathed type K (NiCr/NiAl)
  • Fixed positions
Sample dimensions
  • 10 x 10 mm
  • Ø: 12.7 to 25.4 mm 
  • Length x width: 12.7 to 25.4 mm x 2.0 to 25.4 mm
  • Thickness: 100 nm to 3 mm, depending on the thermophysical properties
Sample geometriesSquare, round, rectangular, strips
Seebeck coefficient range
  • 10 to 2000 μV/K
  • Accuracy*: ±7%
  • Repeatability*: ±3%
Electrical conductivity range
  • 0.05 to 150000 S/cm
  • Accuracy*: ±5%
  • Repeatability*: ±3%
Quality check for electrical conductivityPrior to and during measurement
Quality check for Seebeck measurementPrior to and during measurement
Number of readings automatically averaged≥ 100
AtmosphereInert, oxidizing, reducing (max. 2% H2)
Vacuum-tightness10-2 mbar
SoftwareBased on Windows 7, 32-/64-bit

Find out even more:

The new plug-and-measure feature offers convenient sample change. The operator may now use various sample geometries in different dimensions. Since distance determination between the thermocouples is no longer required, a quick start to the measurement can be realized.

In every respect, the robust design of the SBA 458 Nemesis® allows for unfettered, easy handling. The thermocouples are exceptionally well protected against damage by virtue of Inconel sheathing, and are additionally mechanically fixated in order to yield high precision and reproducibility of the measurement results. Nevertheless, thermocouples and current pins can still be easily replaced by the operator.

The system comes with two micro heaters which operate in alternation. The cyclic heating process is used to perform a quality check for the Seebeck coefficient. A quality check for measurement of electrical conductivity can also be carried out. The user obtains information about the measurement’s performance already while it is still in progress.

Distance determination between fixed thermocouple positions is a cumbersome process which is usually necessary, but this instrument eliminates the need for any operator handling in this regard. By excluding this potential source of error from the determination process for electrical conductivity, the precision and reproducibility of the results are increased.

The hallmark of the SBA 458 Nemesis® is its one-of-a-kind measurement setup which allows more sample geometries than usual for this technique. Depending on the sensor, measurements can be carried out between room temperature and 800°C or room temperature and 1100°C.

With the SBA 458 Nemesis®, it is no longer necessary to use tools to insert and remove the sample. This makes changing the sample fast and easy while preventing any sample damage which might have resulted from sticking to the electrodes. 

Customer support representative at a computer, smiling and engaged, highlighting NETZSCH's commitment to service excellence.


Proven Excellence in Service

At NETZSCH Analyzing & Testing, we offer a comprehensive range of services globally to ensure the optimal performance and longevity of your thermoanalytical equipment. With a track record of proven excellence, our services are designed to maximize the effectiveness of your devices, extend their lifespan, and minimize downtime. 

Unlock the full potential of your equipment with our tailored solutions, backed by years of industry expertise and innovation.

Software

All software features at a glance

Blue digital circuit board featuring a central processing unit (CPU) with three gear icons, symbolizing technology and innovation.

The software is based on Windows 7, 64 bit. It fully controls the measurements, which are performed at each specified temperature interval. The software allows for easy operation and control of the data.

The resistance (U-I plot) and quality check (Seebeck) functions are integrated. The measurement data can be easily exported.

A red Formula 1 car is in a pit stop surrounded by team members clad in red and black uniforms, focusing on a swift tire change.

Consultancy & Sales

Do you have further questions about the instrument or the method and would like to speak to a sales representative?

Service & Support

Do you already have an instrument and need technical support or spare parts?

Downloads and Media

AI Overview
An error occurred. Please try again.