NETZSCH STA 449 Jupiter® thermal analysis instrument with touchscreen display and dual sample carrier, ideal for simultaneous DSC-TGA measurements.
Simultaneous Thermogravimetry

STA 449 F3 Jupiter®

Fascinating Flexibility in Thermal Analysis 

The simultaneous thermal analyzer NETZSCH STA 449 F3  Jupiter® allows the measurement of mass changes and thermal effects between -150°C and 2400°C.

The high flexibility caused by the various sensors, the great variety of sample crucibles and the wide TGA-measuring range make the system applicable for analysis of all kinds of materials including also inhomogenous substances. Easily interchangeable sample holders allow the optimal system adaption to the diverse application areas (TGA, TGA-DTA and TGA-DSC measurements). Various furnaces, easy interchangeable by the user, cover the complete temperature range (please see accessories).
Through to the vacuum tight design measurements at defined atmospheres (e.g. inert) are possible. The system is controlled by a newly developed integrated digital electronic device. The analysis of measuring data runs under a standard PC and the well-proven Windows® software.

Request a Quote

Get a personalized offer now.

Request a Quote

Technical Data

Temperature range
-150°C to 2400°C
Tungsten furnace 
RT to 2400°C
High-speed furnace
RT to 1250°C
NETZSCH STA 449 Jupiter® thermal analysis instrument with digital display, ideal for simultaneous DSC-TGA measurements.

Heating and cooling rates:
0.001 K/min to 50 K/min
(dependent on furnace)

Weighing range:
35000 mg

TG resolution:
0,1 µg (over entire weighing range)

DSC resolution (depending on sensor type):
e.g. < 1 µW for DSC sensor type S and 0.5 µW for DSC sensor type E

Atmospheres:
inert, oxidizing, reducing, static, dynamic

Switch valve: 
for 2 purge gases and 1 protective gas

Vacuum-tight assembly:
up to 10-4 mbar

Coupling:
FT-IR, MS via Capillary or SKIMMER coupling

NETZSCH STA 449 Jupiter® thermal analysis instrument featuring dual measure capability and a digital display for precise data.
TypeTemperature rangeCooling system
Silver furnace-120°C to 675°Cliquid nitrogen
Copper furnace-150°C to 500°Cliquid nitrogen
Steel furnace -150°C to 1000°Cliquid nitrogen
Platinum furnaceRT to 1500°Cforced air
Silicon carbide furnaceRT to 1600°Cforced air
Rhodium furnaceRT to 1650°Cforced air
Graphite furnaceRT to 2000°Ctap or chilled water
Water vapor furnaceRT to 1250°Cforced air
High-speed furnaceRT to 1250°Cforced air
Tungsten furnaceRT to 2400°Ctap or chilled water
Diagram of the STA 449 Jupiter® simultaneous DSC-TGA system, detailing components like the heating element, sample carrier, and gas supply unit.

The STA 449 F3 Jupiter® runs under Proteus® Software on Windows® 7, Windows® 8.1 and Windows®  10. The Proteus® Software includes everything you need to carry out a measurement and evaluate the resulting data. Through the combination of easy-to-understand menus and automated routines, a tool has been created that is extremely user-friendly and, at the same time, allows sophisticated analysis. The Proteus®® software is licensed with the instrument and can of course be installed on other computer systems.

TGA features:

  • Mass changes in wt% or mg
  • Automatic evaluation of mass-change steps
  • Determination of residual mass
  • Extrapolated onset and end temperatures
  • Peak temperatures of the 1st and 2nd derivative of the mass-change curve
  • Automatic baseline and buoyancy correction
  • c-DTA®® for calculated DTA signal with evaluation of characteristic temperatures and the peak area (optional for TGA measurements)

 

DSC features:

You can use the following software with this product

A variety of sample crucibles (pans) made of alumina, platinum, aluminum, graphite, fused silica, etc. is available in different sizes.

The water vapor furnace with perfectly balanced accessories for steam generation, gas mixing and flow control offers the unique opportunity to study the mass and energy changes in samples up to 1250°C under defined absolute humidity.

The high-speed furnace does not require a stand-alone instrument but extends the well-established instrument series STA-Jupiter® by another furnace type. The concept allows for equipping a measuring instrument with a double-furnace hoisting device for two furnaces. The high-speed furnace can therefore be mounted on the double hoisting device combined with other furnaces. Instead of a second furnace, an automatic sample changer (ASC) can optionally be used for the high-speed furnace. Modular flexibility and particularly the combinability of the high-speed furnace with the ASC saves a great amount of time and thus directly results in an increased sample throughput.

Various sample carriers and accessories for the STA 449 F3 Jupiter®, including metallic and colored caps.
STA 449 F3 Jupiter® accessories
White STA 449 sample carrier with a cylindrical base, designed for precise measurements in thermal analysis.
Examples for STA 449 sample carrier and sensor types
Jupiter® simultaneous DSC-TGA sample carrier with dual connectors for efficient sample handling in thermal analysis.
Jupiter® simultaneous DSC-TGA sample carrier featuring dual sample holders for efficient thermal analysis.

Optionally available, the OTS® system allows for reducing effectively the oxygen partial pressure at the sample vicinity.

The automatic sample changer is designed for routine measurements. It works day and night, giving you time for other tasks, and provides for optimal use of the STA 449 F3 Jupiter® (e.g. calibrations on the weekend).

A carousel is available for up to 20 sample and reference crucibles (pans) which can be automatically run in any order. The controlled generation of the required gas atmosphere in the sample chamber and cooling are automatic.

Of course, each sample can be assigned an individual measurement and evaluation macro. Easy-to-understand input masks lead you through the programming of the measurement series. And it is always possible to insert unplanned analyses into a preprogrammed series of measurements that is already in progress.

 

PulseTA®

With the PulseTA® technique an exactly defined quantity of gas is injected to the purge gas of the thermobalance (TGA) or the simultaneous thermal analysis instrument (STA).

This clearly increases the measuring possibilities:

  • Defined/incremental chemical reactions or adsorption of the injection gas with the sample
  • Quantification of gases evolved from the sample.
Flow diagram of gas analysis system, illustrating components for injected gas, purge gas, pulse device, thermal analysis (TA), and mass/FT-IR detection.

Crucibles (Pans) Made of Aluminum for the STA 449 F1 /F3 Jupiter®

Material
(Purity)
Temperature
Range
Consisting ofDimension/
Volume
RemarksOrder Number
Al (99.5%)Max. 600°CCrucible + lidø 6 mm / 25/40 μlSet of 100, cold weldable*6.239.2-64.5.00
Al (99.5%)Max. 600°CCrucible + lidø 6 mm / 25/40 μlSet of 500, cold weldable*6.239.2-64.51.00
Al (99.5%)Max. 600°CCrucible + punched lid (0.05mm)ø 6 mm / 40 μlSet of 100, cold weldable*6.239.2-64.8.00
Al (99.5%)Max. 600°CCrucible + punched lid (0.05mm)ø 6 mm / 40 μlSet of 500, cold weldable*6.239.2-64.81.00
Al (99.5%)Max. 600°CCrucibleø 6.7 mm / 85 μlSet of 100 pieces,
non-weldable
NGB810405
Al (99.5%)Max. 600°CLid Set of 100 pieces, for
NGB810405
NGB810406

* Please note: One and the same sealing press is capable of sealing all the Al crucibles (pan + lid), order no. 6.240.10-80.0.00A

Laboratory setting with scientists in white coats working with advanced equipment, highlighting innovation and quality in research.

This instrument is LabV®️-primed

LabV® takes the data from your analytical instrument: It automatically imports all measurement data into a central and secure database solution, the LabV® software. This allows you to visualize the data in LabV®️ and to make them searchable. Your data will now be accessible from anywhere. Moreover you have the possibility to generate reports.

Product Information

We do not only promise quality, but also individual consulting. Let us start your project together.

Request Information

Videos

Please accept Marketing Cookies to see that Video.

STA 449 F3  Jupiter® Simultaneous DSC-TGA sample carrier change

Please accept Marketing Cookies to see that Video.

Part 2 Sample Preparation Influencing Factors How to Setup an STA Measurement

You may also be interested in

AI Overview
An error occurred. Please try again.