NETZSCH STA 449, a thermal analysis system for safe hydrogen measurements, featuring advanced safety and measurement capabilities.
Simultaneous Thermal Analysis

H2Secure Concept

Safe Examination of Materials Under Hydrogen

Thermal Analysis under Hydrogen

The Key to a Better Understanding of Material Interactions

Hydrogen (H2) is gaining attention for its potential role in sustainable practices and green technology. Research into the interaction of materials with hydrogen is critical for developing eco-friendly solutions that can significantly reduce environmental impact.

One notable application is the use of hydrogen to mitigate highCO2 emissions from metallurgical processes through direct reduction, such as in iron ore reduction. Chemical hydrogen storage, particularly through the use of metal hydrides, is another important avenue of research. Scientists are working to enhance volumetric and gravimetric capacities, as well as hydrogen adsorption/desorption kinetics and the life cycle of potential material candidates. Improving these aspects of materials can lead to more efficient and practical hydrogen storage solutions, which are vital for various applications including transportation, energy storage, and renewable energy systems.

Close-up of green leaves with water droplets, symbolizing sustainability and eco-friendly practices in hydrogen research.

Safe Measurements in Reducing or Oxidizing Atmospheres

The H₂Secure concept developed by NETZSCH features a complete solution for conducting tests in environments with varying concentrations of hydrogen while providing utmost safety. This concept enables safe experimentation in a 100%H2 environment or with lower concentrations ofH2 mixed with non-flammable gases such as nitrogen (N2) or argon (Ar) atmospheres. This flexibility is achieved through a comprehensive safety protocol embedded in the system.

One of the key features of the H₂Secureconcept is its ability to seamlessly perform complex OxidationOxidation can describe different processes in the context of thermal analysis.oxidation-reduction cycles. This involves switching between hydrogen- and oxygen-containing atmospheres within a single measurement, allowing for precise analysis of reaction kinetics and material behavior under different conditions. During these tests, it is crucial to maintain safety at all times. Therefore, in an intermediate state, the sample and testing apparatus are purged with inert gas. This purging process continues until safe conditions are reached for a gas change, minimizing any potential risks associated with handling hydrogen or oxygen.

The NETZSCH H₂Secure concept is TÜV-certified.

The STA Masterclass:
Your Monthly STA Webinar Series

Our webinar series brings you practical, application-first sessions on STA - from phase changes to OxidationOxidation can describe different processes in the context of thermal analysis.oxidation. Learn directly from NETZSCH experts and enhance your daily analysis work.

Explore All Webinars

Method

NETZSCH STA 509 Jupiter, a thermal analysis instrument, designed for safe hydrogen measurements and material interaction analysis.

Simultaneous Thermal Analysis

Simultaneous Thermogravimetry – Differential Scanning Calorimetry

Simultaneous Thermal Analysis (STA) is a method used to analyze the Thermal StabilityA material is thermally stable if it does not decompose under the influence of temperature. One way to determine the thermal stability of a substance is to use a TGA (thermogravimetric analyzer). thermal stability and composition of materials. It combines two techniques: Thermogravimetric Analysis (TGA) and Differential Scanning Calorimetry (DSC).

TGA measures the weight change of a material when it is heated or cooled, providing information on Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition temperatures, moisture content, and Thermal StabilityA material is thermally stable if it does not decompose under the influence of temperature. One way to determine the thermal stability of a substance is to use a TGA (thermogravimetric analyzer). thermal stability. DSC measures the amount of heat required to increase the temperature of a sample, providing insights into Phase TransitionsThe term phase transition (or phase change) is most commonly used to describe transitions between the solid, liquid and gaseous states.phase transitions, heat capacity, and reaction enthalpies.

Thermomechanical Analysis

Thermomechanical analysis (TMA) is a technique for determining the dimensional changes in solids, liquids or pasty materials as a function of temperature and/or time under a defined mechanical force (DIN 51005, ASTM E 831, ASTM D696, ASTM D3386, ISO 11359 – Parts 1 to 3). Itis closely related to dilatometry, which determines the length change of specimens under negligible load (DIN 51045).

NETZSCH TMA 512 Hyperion system for simultaneous thermal analysis, featuring advanced safety for hydrogen measurements.

H₂Secure Concept

Smiling man in a purple plaid shirt stands in a bright kitchen, exuding warmth and approachability.
  • The volume ofH2 is precisely regulated by introducing hydrogen at the top of the furnace and confining it to a defined space above the continuously purged balance chamber.
  • Gas concentrations ofH2 andO2 are continuously measured for safe handling.
  • The central communication unit, the H₂Secure box, processes the overall information and controls the gas flows on the basis of pre-defined safety limits.
  • Fail-safe operation is achieved by opening the magnetic valves in the event of a power failure, thus releasing an inert gas that removes the hydrogen from the system.

set Up of the H₂Secure Concept

Concept for the STA 509 Series

NETZSCH STA 509 Jupiter, a thermal analysis system for safe hydrogen measurements in materials research, featuring user-friendly controls.
H₂Secure Box
Hydrogen Gas Supply
Optimized Gas Path
Monitoring of Gas Concentrations

set Up of the H₂Secure Concept

Concept for the TMA 512 Hyperion®

Advanced thermal analysis equipment for hydrogen testing, featuring precise controls and safety mechanisms for material examination.
H₂Secure Box
Hydrogen Gas Supply
Optimized Gas Path
Monitoring of Gas Concentrations

Specifications

H₂Securefor STA 449/509H₂Securefor TMA 512
Furnace type supporting H₂ measurementsSiCSiC
Temperature rangeRT to 1600°CRT to 1600°C
Sensor types*
  • TGA
  • TGA-DTA
  • TGA-DSC
Thermocouple types*
  • P
  • S
  • B
  • D
  • S
Sensor type for reduction experiments onlyW
Optional 4-fold MFC

Possible switching between hydrogen and

air atmospheres in one measurement

Possible switching between hydrogen and

air atmospheres in one measurement

Hydrogen supply

Supplied by the operator, e.g., hydrogen

generator, H₂ cylinder

supplied by the operator, e.g., hydrogen

generator, H₂ cylinder

H₂ and O₂ measuring cellIncludedincluded
H₂Secure BoxIncludedincluded
Optional gas outlet treatmentH₂ dilutionh₂ dilution
Upgrade of previous modelsPossibleOn request

* Possibility of reduced life time depending on experimental parameters.

NETZSCH STA 449 Jupiter instrument with H₂ icon, illustrating simultaneous thermal analysis for safe hydrogen testing.

Upgrade for the STA 449 Series

The H₂Secure concept is readily accessible for all instruments of the STA 449 and 509 series, offering the flexibility of upgrading existing instruments. Upgraded instruments retain their complete functionality while also enabling safe operations with hydrogen. The upgrade encompasses all essential components and can be conveniently performed on-site by our service team.

Videos

Please accept Marketing Cookies to see that Video.

This is an excerpt from the NETZSCH Tech Talk Spring 2024.