DSC 204 F1 Nevio
Precise and Reliable DSC Results for Pharmaceuticals, Foods and Cosmetics
…by means of the DSC 204 F1 Nevio, the premium differential scanning calorimeter for research and development, material characterization and contract testing.
The instrument serves for the investigation of:
- Melting Temperatures and EnthalpiesThe enthalpy of fusion of a substance, also known as latent heat, is a measure of the energy input, typically heat, which is necessary to convert a substance from solid to liquid state. The melting point of a substance is the temperature at which it changes state from solid (crystalline) to liquid (isotropic melt).Melting temperatures and enthalpies of fusion
- PolymorphismPolymorphism is the ability of a solid material to form different crystalline structures (synonyms: forms, modifications).Polymorphism (ability of a solid substance to exist in multiple forms or crystal structures)
- CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.Crystallization temperatures and enthalpies
- Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.Glass transitions (characteristic for amorphous areas or amorphous substances)
- Solid-solid interactions (e.g., between ingredients in a physical mixture)
- Phase diagrams
- Eutectic PurityA eutectic system is a homogeneous mixture of 2 components that melts and solidifies like a pure substance.Eutectic purity
- Solid-fat content (SFC)
- Reaction temperatures and enthalpies
- Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.Specific heat capacity (cp)
- Curing (Crosslinking Reactions)Literally translated, the term “crosslinking“ means “cross networking”. In the chemical context, it is used for reactions in which molecules are linked together by introducing covalent bonds and forming three-dimensional networks.Cross-linking reactions (Curing (Crosslinking Reactions)Literally translated, the term “crosslinking“ means “cross networking”. In the chemical context, it is used for reactions in which molecules are linked together by introducing covalent bonds and forming three-dimensional networks.curing)
- OxidationOxidation can describe different processes in the context of thermal analysis.Oxidation-induction time and temperature (Oxidative-Induction Time (OIT) and Oxidative-Onset Temperature (OOT)Oxidative Induction Time (isothermal OIT) is a relative measure of the resistance of a (stabilized) material to oxidative decomposition. Oxidative-Induction Temperature (dynamic OIT) or Oxidative-Onset Temperature (OOT) is a relative measure of the resistance of a (stabilized) material to oxidative decomposition.OIT (IsothermalTests at controlled and constant temperature are called isothermal.isothermal), Oxidative-Induction Time (OIT) and Oxidative-Onset Temperature (OOT)Oxidative Induction Time (isothermal OIT) is a relative measure of the resistance of a (stabilized) material to oxidative decomposition. Oxidative-Induction Temperature (dynamic OIT) or Oxidative-Onset Temperature (OOT) is a relative measure of the resistance of a (stabilized) material to oxidative decomposition.OIT (dynamic), Oxidative-Induction Time (OIT) and Oxidative-Onset Temperature (OOT)Oxidative Induction Time (isothermal OIT) is a relative measure of the resistance of a (stabilized) material to oxidative decomposition. Oxidative-Induction Temperature (dynamic OIT) or Oxidative-Onset Temperature (OOT) is a relative measure of the resistance of a (stabilized) material to oxidative decomposition.OOT)
Features of the DSC 204 F1 Nevio:
Software which actively supports you – AutoEvaluation and Identify
AutoEvaluation is the first truly self-acting software feature in thermal analysis. Intelligent algorithms are able to detect and evaluate thermal effects without any user intervention.
Identify is software for curve recognition and interpretation via database comparison. It can manage measurements (also those of a customer’s own), literature data and classes. Numerous libraries are already included, amongst them also one containing data related to the fields of pharmacy, food and cosmetics.
All set for the future – various sensor types
The DSC 204 F1 Nevio can be equipped with different sensors to adapt the instrument to different application needs.
Excellent sensitivity and high resolution
With a value of more than 160 mW/K, the DSC 204 F1 Nevio with t sensor exhibits the highest indium response ratio on the market. This height-to-width ratio of an indium melting peak is an ideal criterion for describing the sensor performance.
Automatic sample tray identification
The instrument can be fitted with an automatic sample changer (ASC, optional) for measuring up to 192 samples plus up to 12 calibration materials or empty pans. If a new sample tray is inserted, the system recognizes the tray and its content automatically via an imprinted 2-D code.
Additionally, the optional piercing device perforates the lids of aluminum pans shortly before a given measurement starts.
Measuring methods independent of instrument
Measurement methods (which can comprise not only temperature programs but also evaluation of the resulting curve) can be used on each device of the same type and comparable configuration. This is particularly advantageous if several DSCs of the Nevio line (DSC 204 F1 or DSC 214 instruments) are installed in the lab.
Efficient and cost-effective cooling
In pharmacy, cosmetics and food, most DSC instruments are equipped with a mechanical cooling system (intracooler). However, if very low start temperatures are required, a liquid nitrogen cooling device can be simultaneously connected to the DSC 204 F1 Nevio. In this case, the LN2 cooling will only be activated at temperatures below -85°C, which reduces the liquid nitrogen consumption considerably.
The Proteus® Protect software meets the requirements of 21 CFR Part 11.
Technical Data

Enthalpy accuracy:
< 1%1)
TGA resolution:
n/a
Indium Response Ratio (*):
> 160 mW/K2)
Exchangeable sensors:
Yes
Cooling options:
Air compressor: RT to 700°C
Compressed air: < 0°C to 700°C
Intracooler: -85°C to 600°C
Liquid nitrogen: -180°C to 700°C
Gas atmospheres:
Inert, oxidizing, static and dynamic
1) for indium
2) using the equation published by B. Wunderlich, Thermal Analysis of Polymeric Materials, Springer (2005), page 346
Gas-tight/vacuum-tight:
Gas-tight
Mass flow controller for purge/protective gas:
3, integrated (0 to 250 ml/min)
Automatic Sample Changer (ASC):
Yes (optional)
Software:
min. Proteus® 8
Advanced Software extensions (optional):
Peak Separation
Kinetics Neo
Thermal Simulations
Size (W x H x D) – incl. ASC, without physical connections:
620 mm x 415 mm x 550 mm

Application Literature
Our latest blog articles
- 18.11.2026
Understanding Citric Acid Decomposition: Deeper Insights with STA-FT-IR Analysis

- 07.10.2026
From the Green Body to a Dense Ceramic – How NETZSCH Termica Neo Makes Sintering Transparent

- 03.10.2026
What DSC Can Reveal About Aging in Polypropylene

- 22.09.2026
NETZSCH Analysis Instruments in Use at South Korean Research Institutes

- 09.09.2026
Introduction to the Rheology of Dispersions – Fundamentals, Influencing Factors and Measurement Methods

- 04.08.2026
Can Artificial Cartilage Behave Like the Real Thing? Rheology Provides the Answer