TMA Analysis for Polymers
Polymers undergo changes in their thermomechanical properties during heating and cooling. TMA analyses can give insights into molecular orientation and quenching effects during cooling. It allows the design of adhesives and other hybrid joints and quality control of shrink films. TMA analyses can hereby provide valuable insight into the composition, structure, production conditions or application possibilities for various materials.

Explore the Five-Part DIL & TMA Webinar Series
Determination of Viscoelastic Properties like Relaxation, Creep and Stress/Strain
The TMA 402 F3 Hyperion® Polymer Edition now offers not only to keep the force constant and to measure the length change, but also to change the displacement and measure the corresponding force. This is for example used in a StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress RelaxationWhen a constant strain is applied to a rubber compound, the force necessary to maintain that strain is not constant but decreases with time; this behavior is known as stress relaxation. The process responsible for stress relaxation can be physical or chemical, and under normal conditions, both will occur at the same time. relaxation test. Here, a sample is stretched by a specific amount at a defined temperature. During the test, the deformation is kept constant and the progression of the force is recorded. This force continuously decreases as a result of material RelaxationWhen a constant strain is applied to a rubber compound, the force necessary to maintain that strain is not constant but decreases with time; this behavior is known as stress relaxation. The process responsible for stress relaxation can be physical or chemical, and under normal conditions, both will occur at the same time. relaxation. StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.Stress-RelaxationWhen a constant strain is applied to a rubber compound, the force necessary to maintain that strain is not constant but decreases with time; this behavior is known as stress relaxation. The process responsible for stress relaxation can be physical or chemical, and under normal conditions, both will occur at the same time. relaxation is ultimately defined by the residual StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress measured after a defined exposure period. The data can be depicted graphically in a StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress-time diagram. It is then possible to read off both the StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress-RelaxationWhen a constant strain is applied to a rubber compound, the force necessary to maintain that strain is not constant but decreases with time; this behavior is known as stress relaxation. The process responsible for stress relaxation can be physical or chemical, and under normal conditions, both will occur at the same time. relaxation behavior and the values for the RelaxationWhen a constant strain is applied to a rubber compound, the force necessary to maintain that strain is not constant but decreases with time; this behavior is known as stress relaxation. The process responsible for stress relaxation can be physical or chemical, and under normal conditions, both will occur at the same time. relaxation rate and time.
Mechanical Cooling to -70°C
The TMA 402 F3 Hyperion® Polymer Edition is specifically designed for polymer applications. It comes with a compact, highly reactive furnace capable of covering a temperature range from -70°C to 450°C using a mechanical cooling system without the need for LN₂.

Request a Quote
Technical Data
IC Furnace
Heating rates
Measuring ranges/
Δl resolution
5000 μm (± 2500 μm) / 1.25 nm

Displacement Control
Displacement static, steps, ramps
Force range (load at sample)
0.001 N to 3 N without using additional weights
Force resolution
< 0.01 mN
Interchangeable sample holder systems
Fused silica, up to 450°C
Sample dimensions
Expansion/penetration: length: 30 mm max.; sample holder Ø 8 mm
Tension: length: 30 mm max.; width: 6 mm; thickness: 1 mm
3-Point bending: length: 10 mm max.; width: 5 mm
Automatic sample length determination (precision: 0.01 mm)
Atmospheres
1 mass flow controller (MFC, 2nd independent MFC optional), gas flow rate 0 to 250 ml/min software-controlled, inert, oxidizing, reducing, vacuum (10-4 mbar)
Various accessories
Spacers, crucibles and special wax containers