Materiały nieorganiczne
Neodymsulfate Pentahydrate - Evolved Gas Analysis (QMS)
Nd2 (SO4)3*5H2O (29.53 mg) was heated at a rate of 10 K/min up to 1400°C in a nitrogen flow.
The MID curves, directly imported from the coupled QMS 403 Aëolos® Quadro, show the well separated gas evolution for water, oxygen and sulfur dioxide in perfect correlation with the TG steps.