13.02.2020 by Milena Riedl

How to Analyze Automotive Thermoplastic Parts for Failure

A person stands in the center of a complex, white maze, symbolizing challenges in analyzing thermoplastic part failures.

Thermoplastic parts can fail. This is no secret. However, when it has happened it is crucial to find out the reason for the failure of a part. Here is a short list of thermal analysis techniques and which questions they can answer in your failure analysis.

Thermoplastic parts can fail. This is no secret. However, when it has happened it is crucial to find out the reason for the failure of a part. Then, removing the cause of defect takes priority.

For the analysis of the cause of failure of injection-molded thermoplastic parts, a superior level of expertise in material science, production methods and analytical instrumentation is required. There is a wide array of failure scenarios that can occur. Possibilities range from misuse and unintentional service conditions to design faults, molding issues, StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress, overload and degradation.

Thermal analysis instruments are powerful tools for failure analysis. Here is a short list of thermal analysis techniques and which questions they can answer in your failure analysis:

Thermogravimetric Analysis

  • Was the material filled with the right amount of fillers, plasticizer and modifiers?
  • Was the material thermally stable to withstand service temperatures?
  • Did the material absorb water?
NETZSCH TG 209 Libra thermal analysis instrument for evaluating automotive thermoplastic part failures and stability.
Temperature-dependent predictions of polymer degradation over time, illustrated by dynamic TGA measurement curves.

Dynamic-Mechanical Analysis

  • Did the material have the same mechanical properties at service temperatures?
  • Did the material degrade at a faster rate than anticipated?
  • Did the material lose its mechanical properties due to liquid interactions?

These few questions give you a short overview of the wide field of questions in failure analysis that can be answered with thermal analysis instrumentation.

We will continue talking about failure analysis!