Lithium-ion batteries arranged in front of icons of renewable energy sources, highlighting advancements in sustainable technology.

03.09.2025 by Aileen Sammler

Improving Lithium-Ion Battery Safety: Thermal and Kinetic Analysis of LiPF₆ Electrolytes with the NETZSCH DSC & Kinetics Neo

Discover how Differential Scanning Calorimetry (DSC) and the Kinetics Neo software by NETZSCH improve lithium-ion battery safety by analyzing the thermal and kinetic stability of LiPF₆-based electrolytes and prevent Thermal runawayA thermal runaway is the situation where a chemical reactor is out of control with respect to temperature and/or pressure production caused by the chemical reaction itself. Simulation of a thermal runaway is usually carried out using a calorimeter device according to accelerated rate calorimetry (ARC).thermal runaway and optimize performance.

Lithium-ion batteries (LIBs) power our smartphones, electric vehicles, and renewable energy storage systems. As the global demand increases rapidly, safety and reliability have become top priorities. Regulatory frameworks such as the EU Battery Regulation 2023 and international standards now impose strict requirements on battery thermal safety testing.

At the heart of every LIB is the electrolyte, and one of the most widely used salts in carbonate solvents is LiPF₆. Although LiPF₆ features excellent Ionic conductivity and compatibility with graphite anodes, it is thermally and chemically instable. This instability can trigger Thermal runawayA thermal runaway is the situation where a chemical reactor is out of control with respect to temperature and/or pressure production caused by the chemical reaction itself. Simulation of a thermal runaway is usually carried out using a calorimeter device according to accelerated rate calorimetry (ARC).thermal runaway, a major safety concern in electric mobility and stationary storage.

To address these challenges, researchers and manufacturers rely on advanced material characterization. In this new application note, a NETZSCH DSC combined with the Kinetics Neo software was used to analyze the Thermal StabilityA material is thermally stable if it does not decompose under the influence of temperature. One way to determine the thermal stability of a substance is to use a TGA (thermogravimetric analyzer). thermal stability and Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition kinetics of LiPF₆-based electrolytes.

Key Results from the Study

Thermal Events Identified by DSC

A NETZSCH DSC was used to analyze LiPF₆ in a mixed carbonate solvent system (EMC+DMC+EC, 1:1:1). The following thermal effects were detected above 190°C:


Kinetic Analysis with Kinetics Neo Software

  • Kinetic evaluation confirmed a three-step reaction model with activation energies of 146.3, 137.2, and 118.6 kJ/mol.
  • The correlation between the measured and calculated data reached R² = 0.997, indicating an excellent agreement between experimental and simulated data


Predictions for Real-Life Scenarios

Why It Matters for Today’s Battery Industry

By combining Differential Scanning Calorimetry (DSC) and Kinetics Neo, NETZSCH provides a powerful toolkit for predicting electrolyte behavior under real operating and abuse conditions.

Benefits of the NETZSCH DSC for Battery Research

The NETZSCH DSC 300 Caliris® analysis instrument features exceptional sensitivity and flexibility, making it the ideal tool for analyzing battery electrolytes and materials. 

In the context of lithium-ion battery safety, DSC enables researchers to precisely determine Phase TransitionsThe term phase transition (or phase change) is most commonly used to describe transitions between the solid, liquid and gaseous states.phase transitions, Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition temperatures, and heat-flow events that are critical for identifying the onset of Thermal runawayA thermal runaway is the situation where a chemical reactor is out of control with respect to temperature and/or pressure production caused by the chemical reaction itself. Simulation of a thermal runaway is usually carried out using a calorimeter device according to accelerated rate calorimetry (ARC).thermal runaway. With its modular design and high-pressure crucibles, the DSC Caliris® allows for reliable results, even for volatile electrolyte systems.

NETZSCH DSC 300 Caliris, a thermal analysis instrument, used for lithium-ion battery safety research and thermal stability testing.
The NETZSCH DSC 300 Caliris® Classic
NETZSCH DSC 300 Caliris Classic, an advanced thermal analyzer for efficient lithium-ion battery electrolyte testing and safety evaluation.
The Logo of NETZSCH Kinetics Neo Software

Benefits of Kinetics Neo in Battery Safety Analysis

The Kinetics Neo software extends DSC measurements by enabling predictive simulations under real-life conditions. For battery developers, this means that data from a set of three DSC heating experiments can be used to model IsothermalTests at controlled and constant temperature are called isothermal.isothermal storage stability, AdiabaticAdiabatic describes a system or measurement mode without any heat exchange with the surroundings. This mode can be realized using a calorimeter device according to the method of accelerating rate calorimetry (ARC). The main purpose of such a device is to study scenarios and thermal runaway reactions. A short description of the adiabatic mode is “no heat in – no heat out”.adiabatic conditions, and different temperature profiles. 

This allows for accurate predictions of the electrolyte behavior during operation, transport, or abuse scenarios – supporting the design of safer, longer-lasting battery systems.

Conclusion

The combination of NETZSCH DSC and Kinetics Neo software delivers essential insights into the thermal and kinetic stability of LiPF₆-based electrolytes. These results directly support battery developers in preventing Thermal runawayA thermal runaway is the situation where a chemical reactor is out of control with respect to temperature and/or pressure production caused by the chemical reaction itself. Simulation of a thermal runaway is usually carried out using a calorimeter device according to accelerated rate calorimetry (ARC).thermal runaway, ensuring compliance with safety standards, and driving the transition towards safe and sustainable e-mobility and energy storage systems.

? Read the full Application Note here:

Learn more about NETZSCH DSC Instruments and Kinetics Neo Software

  • DSC 300 Caliris® Classic

    Quality assurance of polymers, food, cosmetics and organics

    • Compact design for more space in the lab
    • Temperature range: -170°C to 600°C
    • Automatic Sample Changer: Up to 20 samples and references
  • DSC 300 Caliris® Select

    Quality assurance of polymers, food, cosmetics and organics

    • Choose your appropriate module: Standard, Polymer or High-Performance
    • Temperature range: -180°C to 750°C
    • Automatic Sample Changer: Up to 192 + 12 samples and references
  • DSC 300 Caliris® Supreme

    Quality assurance of polymers, food, cosmetics and organics

    • Three easily interchangeable modules: Standard, Polymer and High-Performance
    • Temperature range: -180°C to 750°C
    • UV-Accessory: Investigate curing reactions with photo-calorimeter

Share this article: