Read about the following topics in this series: From the Kinetic Model to Real-World Applications; Scale-up & Safety; Polymer Curing; Thermoplastic CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.Crystallization (PA12); Ceramic SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. Sintering
Every polymer tells two stories: The one on the DSC curve and the one hidden inside the part
In small samples, Curing (Crosslinking Reactions)Literally translated, the term “crosslinking“ means “cross networking”. In the chemical context, it is used for reactions in which molecules are linked together by introducing covalent bonds and forming three-dimensional networks.curing looks perfect. But inside a real part, heat builds up, reaction fronts move, and vitrification can freeze the reaction long before completion. NETZSCH Termica Neo exposes that invisible world. It transforms kinetic data into 3D maps of temperature, conversion, and reaction rate.
Now, you can see your resin Curing (Crosslinking Reactions)Literally translated, the term “crosslinking“ means “cross networking”. In the chemical context, it is used for reactions in which molecules are linked together by introducing covalent bonds and forming three-dimensional networks.curing in both space and time rather than just along a line.

From Laboratory Curves to Spatial Reality
In the lab, you measure kinetics for small samples with the same temperature. In production, you have sample geometry with temperature gradients inside. The challenge lies between them: how to predict when the center of a laminate, mold, or adhesive layer catches up with its surface without hot spots with too high temperatures leading to material damage.
The Termica Neo software closes that gap by importing Kinetics Neo data – model-free or model-based, single- or multi-step, autocatalytic or diffusion-controlled – and applying it to real component shapes.
Define:
- Material parameters: Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.specific heat capacity, DensityThe mass density is defined as the ratio between mass and volume. density, Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity
- Geometry: plate, cylinder, sphere, or custom rotational body
- Boundary conditions: heat transfer, convection, emissivity
- Temperature program: IsothermalTests at controlled and constant temperature are called isothermal.isothermal, dynamic, step-IsothermalTests at controlled and constant temperature are called isothermal.isothermal, modulated

What Happens During Curing?
As the crosslinking reaction starts, the ExothermicA sample transition or a reaction is exothermic if heat is generated.exothermic heat generated raises the local temperature.
The outer layers heat up faster to surrounding temperature, while the interior firstly remains colder and is then heated by the accelerating reaction and creates hotspots. The glass-transition temperature, Tg, increases above the sample temperature, molecular mobility declines and diffusion control slows the process.
Termica Neo captures these coupled effects simultaneously: temperature ↔ reaction under chemical control↔ reaction under diffusion control.
The result is a living model of the Curing (Crosslinking Reactions)Literally translated, the term “crosslinking“ means “cross networking”. In the chemical context, it is used for reactions in which molecules are linked together by introducing covalent bonds and forming three-dimensional networks.curing front moving through your part.

Case Study: Epoxy Cylinder Curing with Bottom Heating
Simulation of the curing of a simple epoxy cylinder reveals information that cannot be obtained through measurement alone:
- A reaction front travels upwards through the height.
- The axis region lags in conversion and cools slowly.
- Over-curing at the surface and under-curing inside occur in parallel.
By adjusting temperature ramps or hold times on each side of the cylinder in Termica Neo, engineers can eliminate these gradients before the first real molding trial.

From Reactive Guesswork to Predictive Control
Curing is no longer a blind spot. With the NETZSCH Termica Neo software, you can simulate scenarios from lab scale to industrial scale, testing new resin systems, curing cycles, and variations in geometry and volume to accurately predict curing behavior for the prediction of:
- Hotspot location and temperature
- Degree of CureThe degree of curing describes the conversion achieved during crosslinking reactions (curing). Degree of cure (α) distribution
- Presence of diffusion-controlled reaction depending on the local Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.glass transition temperature, Tg
- Optimized process windows with minimal energy input
You achieve efficient processes and high product quality, backed by minimal energy use instead of trial and error.

Benefits of Termica Neo
- Direct kinetic import from Kinetics Neo
- Full 2D/3D visualization of temperature, conversion, and reaction rate
- Simulation of autocatalytic and diffusion-controlled curing
- Geometry-specific optimization for composites, adhesives and coatings
- Reduced trial cycles | Higher process reliability | Lower energy cost
About This Blog Series
This article continues the NETZSCH series: “The New Dimension of Thermal Analysis with Termica Neo: Software for the Thermal Simulation of Chemical Reactions on an Industrial Scale.”
Already published articles: (see links below)
- From Kinetic Model to Real-World Application — turning 1-D data into 3-D insight.
- Scale-up & Safety — predicting runaways before they happen.
- Polymer Curing — How Termica Neo Makes Curing Visible
These articles come next: Thermoplastic CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.Crystallization (PA12) and Ceramic SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. Sintering: Applying the same 3D vision to cooling and densification. Stay tuned!
See Your Curing Process Come to Life. Explore NETZSCH Termica Neo and watch how curing really happens inside your component, not just in your data.
--------------------------
Useful Links:
Get your free demo version:Request Demo Version of Temica Form - NETZSCH Termica Neo
Download the new brochure to learn more:Termica Neo Brochure
Direct contact:Feature Request - NETZSCH Kinetics Neo
Learn even more:Termica Neo - NETZSCH Termica Neo
These webinars could be of interest to you:
These blog articles may also be of interest
- 07.10.2026
From the Green Body to a Dense Ceramic – How NETZSCH Termica Neo Makes Sintering Transparent

- 13.07.2026
Thermoplastic Crystallization – Understanding PA12 During Cooling

- 14.05.2026
Polymer Curing – How NETZSCH Termica Neo Makes Curing Visible

- 03.03.2026
Scale-Up & Safety: How NETZSCH Termica Neo Predicts What Could Go Wrong

- 03.02.2026
From Kinetic Model to Real-World Application: How NETZSCH Termica Neo Simulates Thermal Reactions

- 06.05.2024
NETZSCH Tech Talk – Spring Edition: Unveiling Thermal Innovations in Just 30 Minutes

- 07.02.2024
Introducing Termica Neo: The New NETZSCH Software for Thermal Simulation in Industrial Settings