High-performance NETZSCH GABO Eplexor® testing instrument with dynamic force capabilities up to 500 N for elastomers.
dynamic mechanical analysis

DMA 503 Eplexor® HT up to 500 N

For ceramics, metals, alloys, glasses, composites and more 

Highlights

The DMA 503 Eplexor® HT line is the only instrument series on the market which is able to carry out DMA measurements with a maximum dynamic force of 500 N to 1500°C.

A high-temperature furnaces from RT to 1500°C is available. With a standard furnace (-160°C to 500°C) simultaneously mounted, it is possible to perform consecutive test runs in both the low- and high-temperature range. Eplexor® HT instruments can thus cover the entire temperature span from -160°C to 1500°C.

The electronics within the system automatically identify which furnace is currently in use.

The following DMA 503 Eplexor® HT are available:

Instrument TypeMax. Static ForceMax. Dynamic Force *)
DMA 503 Eplexor® 100 N HT1500 N± 100 N
DMA 503 Eplexor® 150 N HT1500 N± 150 N
DMA 503 Eplexor® 500 N HT1500 N± 500 N

Dynamic Mechanical Analysis: A Five-Part Webinar Series

Learn the fundamentals and advanced applications of Dynamic Mechanical Analysis (DMA) to confidently characterize viscoelastic material behavior, accurately interpret mechanical properties, and optimize material development and processing performance.

Explore All Webinars

Method

The Dynamic Mechanical Thermal Analyzer applies forced periodic loads to the sample and analyzes the phase shift between this primary excitation and the material’s response. The response of an ideal elastic system (e.g., spring) on a sinusoidal load at a given frequency is of the same frequency and exactly in phase with the excitation. The situation changes in a real system: A phase shift (δ > 0°) between the primary excitation and response of the same frequency occurs in the case of linear visco-elastic materials (e.g., polymers).

Graph illustrating dynamic mechanical analysis, showcasing E' and E'' values for various materials like oil, melt, polymer, and metal.
Graph illustrating force and strain amplitudes over time, highlighting dynamic testing principles in elastomers and materials.

Elastic and non-elastic properties inherently describe the dynamic mechanical performance of the material. The storage modulus E’, the real part of the Complex ModulusThe complex modulus consists of two components, the storage and the loss moduli. The storage modulus (or Young’s modulus) describes the stiffness and the loss modulus describes the damping (or viscoelastic) behavior of the corresponding sample using the method of Dynamic Mechanical Analysis (DMA). complex modulus E*, represents the elastic component; the Viscous modulusThe complex modulus (viscous component), loss modulus, or G’’, is the “imaginary” part of the samples the overall complex modulus. This viscous component indicates the liquid like, or out of phase, response of the sample being measurement. loss modulus E’’, the dissipated part, is the imaginary part. Depicted in the complex plane, the loss and storage modulus are the projections of the Complex ModulusThe complex modulus consists of two components, the storage and the loss moduli. The storage modulus (or Young’s modulus) describes the stiffness and the loss modulus describes the damping (or viscoelastic) behavior of the corresponding sample using the method of Dynamic Mechanical Analysis (DMA). complex modulus onto the real and imaginary axis. The tangent of the angle between the real axis and the Complex ModulusThe complex modulus consists of two components, the storage and the loss moduli. The storage modulus (or Young’s modulus) describes the stiffness and the loss modulus describes the damping (or viscoelastic) behavior of the corresponding sample using the method of Dynamic Mechanical Analysis (DMA). complex modulus (E*) represents the phase shift (tanδ) between the two.

Specifications

Technical Data

Temperature Range
-160°C to 1500°C
(two furnaces needed for full temperature range)
Frequency Range
0.0001 Hz to 100 Hz; optional up to 200 Hz for fatigue
Static Force Range
max. 1500 N
  • Dynamic force range: ± 500 N, ± 150 N,  ± 100 N
  • Interchangeable force sensor:  ±10 N to ±2500 N
  • Blade springs: counteract the static forces and allow for independent superposition of the dynamic forces
  • Static displacement: 80 mm (50 mm with furnace)
  • Dynamic displacement: up to ± 6 mm (depending on the DMA 503 Eplexor® model)
  • Measurement modes for applications above 500°C:
    3-point bending, compression, tension (up to 900°C)
  • Work space of the high-temperature furnaces:
    cylindrical chamber, diameter: 70 mm, height: 120 mm

Software

The comprehensive DMA 503 Eplexor® HT Series software is based on Windows operating systems. The extensive software package comprises data and curve analyses, hysteresis representation, master curve calculations, etc. It also includes specific templates for tension, compression or bending tests.

The software features include:

Red race car in a pit stop with crew members in red uniforms working efficiently under sunny conditions.

Consultancy & Sales

Do you have further questions about the device, the method and would you like to speak to a sales representative?

Service & Support

Do you already have an device and need technical support or spare parts?

Downloads & Media

Brochure and Datasheet

Videos

Setting New Standards up to High Forces with our DMA 503 Eplexor®

Our latest instrument offers dynamic force ranges up to 500 N and static loads up to 1500 N, ideal for testing large or stiff samples. Designed for elastomers and reinforced materials, it features flexible roller bearings for bending tests and interchangeable plates for tensile testing. The high-temperature version can reach temperatures up to 1500°C, enabling precise measurements. 

Please accept Marketing Cookies to see that Video.

This is an excerpt of our NETZSCH Tech Talk of December 2024.

Videos & Webcasts

Please accept Marketing Cookies to see that Video.

NETZSCH GABO Eplexor®® 500 N

Please accept Marketing Cookies to see that Video.

Please accept Marketing Cookies to see that Video.

How to test Rubber - Predictive Testing in Tensile Mode - Part 2  

Please accept Marketing Cookies to see that Video.

Predictive Testing in the Tire Industry 

Please accept Marketing Cookies to see that Video.

How to use Segment Program with Eplexor®® 9 Software 

Please accept Marketing Cookies to see that Video.

How to test Rubber - Predictive Testing in Tensile Mode - Part 1  
AI Overview
An error occurred. Please try again.