Highlights
The DMA 503 Eplexor® HT line is the only instrument series on the market which is able to carry out DMA measurements with a maximum dynamic force of 500 N to 1500°C.
A high-temperature furnaces from RT to 1500°C is available. With a standard furnace (-160°C to 500°C) simultaneously mounted, it is possible to perform consecutive test runs in both the low- and high-temperature range. Eplexor® HT instruments can thus cover the entire temperature span from -160°C to 1500°C.
The electronics within the system automatically identify which furnace is currently in use.
The following DMA 503 Eplexor® HT are available:
| Instrument Type | Max. Static Force | Max. Dynamic Force *) |
| DMA 503 Eplexor® 100 N HT | 1500 N | ± 100 N |
| DMA 503 Eplexor® 150 N HT | 1500 N | ± 150 N |
| DMA 503 Eplexor® 500 N HT | 1500 N | ± 500 N |

Dynamic Mechanical Analysis: A Five-Part Webinar Series
Method
The Dynamic Mechanical Thermal Analyzer applies forced periodic loads to the sample and analyzes the phase shift between this primary excitation and the material’s response. The response of an ideal elastic system (e.g., spring) on a sinusoidal load at a given frequency is of the same frequency and exactly in phase with the excitation. The situation changes in a real system: A phase shift (δ > 0°) between the primary excitation and response of the same frequency occurs in the case of linear visco-elastic materials (e.g., polymers).


Elastic and non-elastic properties inherently describe the dynamic mechanical performance of the material. The storage modulus E’, the real part of the Complex ModulusThe complex modulus consists of two components, the storage and the loss moduli. The storage modulus (or Young’s modulus) describes the stiffness and the loss modulus describes the damping (or viscoelastic) behavior of the corresponding sample using the method of Dynamic Mechanical Analysis (DMA). complex modulus E*, represents the elastic component; the Viscous modulusThe complex modulus (viscous component), loss modulus, or G’’, is the “imaginary” part of the samples the overall complex modulus. This viscous component indicates the liquid like, or out of phase, response of the sample being measurement. loss modulus E’’, the dissipated part, is the imaginary part. Depicted in the complex plane, the loss and storage modulus are the projections of the Complex ModulusThe complex modulus consists of two components, the storage and the loss moduli. The storage modulus (or Young’s modulus) describes the stiffness and the loss modulus describes the damping (or viscoelastic) behavior of the corresponding sample using the method of Dynamic Mechanical Analysis (DMA). complex modulus onto the real and imaginary axis. The tangent of the angle between the real axis and the Complex ModulusThe complex modulus consists of two components, the storage and the loss moduli. The storage modulus (or Young’s modulus) describes the stiffness and the loss modulus describes the damping (or viscoelastic) behavior of the corresponding sample using the method of Dynamic Mechanical Analysis (DMA). complex modulus (E*) represents the phase shift (tanδ) between the two.
Specifications
Technical Data
Temperature Range
(two furnaces needed for full temperature range)
Frequency Range
Static Force Range
- Dynamic force range: ± 500 N, ± 150 N, ± 100 N
- Interchangeable force sensor: ±10 N to ±2500 N
- Blade springs: counteract the static forces and allow for independent superposition of the dynamic forces
- Static displacement: 80 mm (50 mm with furnace)
- Dynamic displacement: up to ± 6 mm (depending on the DMA 503 Eplexor® model)
- Measurement modes for applications above 500°C:
3-point bending, compression, tension (up to 900°C) - Work space of the high-temperature furnaces:
cylindrical chamber, diameter: 70 mm, height: 120 mm
Software
The comprehensive DMA 503 Eplexor® HT Series software is based on Windows operating systems. The extensive software package comprises data and curve analyses, hysteresis representation, master curve calculations, etc. It also includes specific templates for tension, compression or bending tests.
The software features include:
- Frequency sweep of 0.0001 Hz to 100 Hz (optional up to 200 Hz for fatigue)
- Temperature sweep (controlled temperature variation at fixed frequency)
- Time sweep from 1 s to 107 s
- Correlated temperature and frequency sweep at IsothermalTests at controlled and constant temperature are called isothermal.isothermal steps
- Correlated dynamic and static StrainStrain describes a deformation of a material, which is loaded mechanically by an external force or stress. Rubber compounds show creep properties, if a static load is applied.strain amplitude sweeps; equidistantly or logarithmically subdivided
- Master curves (TTS, WLF, numeric mastering), segment tests
- Evaluation of Complex ModulusThe complex modulus consists of two components, the storage and the loss moduli. The storage modulus (or Young’s modulus) describes the stiffness and the loss modulus describes the damping (or viscoelastic) behavior of the corresponding sample using the method of Dynamic Mechanical Analysis (DMA). complex modulus (E*, G*), storage modulus (E’, G’), Viscous modulusThe complex modulus (viscous component), loss modulus, or G’’, is the “imaginary” part of the samples the overall complex modulus. This viscous component indicates the liquid like, or out of phase, response of the sample being measurement. loss modulus (E’’, G’’) damping factor (t and δ) by temperature sweeps, StrainStrain describes a deformation of a material, which is loaded mechanically by an external force or stress. Rubber compounds show creep properties, if a static load is applied.strain and force sweeps, time sweeps, Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.glass transition temperature, and optional CreepCreep describes a time and temperature dependent plastic deformation under a constant force. When a constant force is applied to a rubber compound, the initial deformation obtained due to the application of the force is not fixed. The deformation will increase with time.creep, RelaxationWhen a constant strain is applied to a rubber compound, the force necessary to maintain that strain is not constant but decreases with time; this behavior is known as stress relaxation. The process responsible for stress relaxation can be physical or chemical, and under normal conditions, both will occur at the same time. relaxation, fatigue, energy loss, hysteresis, Payne/Mullins effect analysis
- Prediction of the Rolling ResistanceThe rolling resistance is a force resisting the motion when a body is rolling across a surface. This determines the slip resistance of, e.g., car or truck tires.rolling resistance of tires (optional)

Consultancy & Sales
Do you have further questions about the device, the method and would you like to speak to a sales representative?
Service & Support
Do you already have an device and need technical support or spare parts?
Related Devices
Downloads & Media
Brochure and Datasheet
Application Literature
Videos
Setting New Standards up to High Forces with our DMA 503 Eplexor®
Our latest instrument offers dynamic force ranges up to 500 N and static loads up to 1500 N, ideal for testing large or stiff samples. Designed for elastomers and reinforced materials, it features flexible roller bearings for bending tests and interchangeable plates for tensile testing. The high-temperature version can reach temperatures up to 1500°C, enabling precise measurements.