Stainless steel food processing machine with adjustable components, featuring heating elements for efficient cooking.
Fire Testing

TDP 909 T4

For Determining the Performance of Roofs against External Fire Exposure

Highlights

Test 4 with two Stages incorporating burning brands, wind and supplementary radiant heat in accordance with DIN CEN/TS 1187

Convenient Testing of Representative Roof Constructions

The DIN CEN/TS 1187 standard specifies four test methods for determining the fire behavior of roofs when exposed to external fire. The TDP 909 T4 allows for a test in accordance with test method 4. This two-step method assesses the fire behavior of roofs using incendiary devices (burning brands), wind and additional radiant heat. It determines whether and how fire penetrates the roof and the extent of falling or burning material on the rooftop and/or on the underside.

Samples, which are representative for the overall roof structure can be tested in a frame with dimensions of 840 x 840mm2. The tiltable sample holder also allows for the testing of specified roof pitches. The radiant plate can be easily moved from the calibration position to the test position by the joint integrated into the solid steel frame.

Interested in a test in accordance with test method 3?

Two smiling roofers in orange helmets sit on a shingled roof, enjoying a break with tools and a toolbox nearby.

Two-Stage Test Using Simulation of Wind and Radiant Heat

Testing is carried out in two stages, the Preliminary Test (stage 1) and the Burn-Through Test (stage 2). The Preliminary Test determines whether the test sample is ignited by the presence of a simulative incendiary device (burning brands) without being exposed to thermal radiation. The burn-through test adds wind and radiant heat, generated by the fan and the radiant panel, in order to test the burning behavior of the roof sample under realistic conditions.

To classify the test sample, this method investigates - in addition to the duration of the flames - the extent of flame spread, the timing and type of roof penetration, and the occurrence, dripping or falling of burning or molten material.

Features at a Glance

  • Mobile stainless steel base frame with rails as a receptacle for the movable sample carrier trolley
  • Sample carrier trolley with upward-opening sample cover and integrated observation window
  • Two solid opposing steel girder constructions with swivel mechanism for the radiant heater panel, 2 lockable positions (calibration position/test position)
  • High-quality radiant heater, consisting of 4 individual square radiant heater elements. Each 300 mm by 300 mm, heat resistant up to 900°C mounted on a by 45° swivel frame and equipped with four ignition electrodes.
  • Fire simulation by burner lance with pressure reducer and gas connection hose
  • Wind simulation as needed for T4 test by integrated fan
  • Gas supply to the radiant panel via measuring and control unit
  • Measuring and control unit with intuitive touch display for easy user guidance
  • All components can be controlled individually and manually at any time
  • Useful accessories for calibrating the roof fire testing stand are included in the scope of delivery

Specifications

Measurement method

Determination of the performance of roofs exposed to external fire – Test 4

in two stages incorporating incendiary device, wind and supplementary

radiant heat in accordance with DIN CEN/TS 1187

Burner
  • Burner lance; length of 2300 mm
  • Fed with city gas
  • With needle valve, pressure reducer and gas supply hose
Sample holder
  • Mobile sample carrier trolley; stainless steel
  • Semicircular sample cover; opening on the top; stainless steel; with fireproof observation window; slewable
  • Metal sample holding frame
Pit crew preparing a red Formula 1 car for a quick tire change during a race, showcasing teamwork and precision on track.

Consultancy & Sales

Do you have further questions about the instrument or the method and would like to speak to a sales representative?

Service & Support

Do you already have an instrument and need technical support or spare parts?

Downloads and Media

AI Overview
An error occurred. Please try again.