Automated testing chamber with an open door and digital control panel, designed for precision experiments in laboratory settings.
Fire Testing

TSK 906

Smoldering Test Device

Highlights

Testing the vertical flame spread on a core, an insulated conductor or a cable – Test method with a 1 kW flame with a gas/air mixture in accordance with EN 60332-1-2

Overview of functions:

  • Housing to protect the test procedure
  • Housing – stainless steel metal construction in accordance with EN 60332 – 1-1
  • Dimensions of the housing (H x W x D): 1200 x 300 x 450 mm
  • 1 kW propane burner in accordance with standard EN 60695-11-2
  • Burner can be tilted vertically and at 45º to the vertical axi
  • Gas control system with valves and mass flow meters for propane and air
  • Touch display for controlling the burner
  • Software-supported calibration of the 1 kW flame
  • TSK 906 calibration device for 1 kW burner consisting of thermocouple with copper block (10 g)
  • TSK 906 sample holder in accordance with EN 60332-1-2
  • TSK 906 sample holder for calibration device
  • TSK 906 burner gauge in accordance with EN 60332-1-2
  • TSK 906 manual on USB stick

Specifications

Test procedure

The test equipment is suitable for carrying out the tests of vertical flame spread using 1 kW flame of propane-air mixture for a wire or a single insulated line or cable.

The test equipment is also suitable for evaluating falling burning drops/parts, when a wire cable, a cable, a line or a fiber optic cable is subjected to defined fire conditions. – according to EN 60332-1

Dimensions of the test equipment
  • Overall height: 2150 mm
  • Overall width: 1390 mm
  • Overall depth: 1075 mm
Weight of the equipment165 kg
Operating voltage100-230 VAC 50Hz
Exhaust tubeDiameter: 200 mm
Volume chamber1.3 m³
Volume metal shield0.16 m³
Gas system
  • Mass Flow Controller for propane
    Supply: propane gas with a purity of at least 98%
    Flow rate: 0.016 – 0.8 nl/minC3H8 (Propane) at 20°C
  • Mass Flow Controller for air
    Supply: air
    Flow rate: 0.24 – 12nl/min AIR at 20°C
Calibration device
  • Diameter: 9 mm
  • Weight: 10 (+/- 0.05) g
  • Material: Electrolytic copper CU-ETP USN C11000
Thermocouple
  • Type K Thermocouple
    Sheath material for at least 1250°C
  • Limits of the thermocouple by class 1
Scope of delivery
  • 1x TSK 906 Test equipment according to EN 60332-1
  • 1 x Touch display for burner control and calibration
  • 1 x TSK 906 calibration device for 1KW burner consisting of thermocouple with copper block (10g)
  • 1 x TSK 906 sample holder according to EN 60332-1-2
  • 1 x TSK 906 sample holder for calibration unit
  • 1 x TSK 906 burner gauge according to EN 60332-1-2
  • 1 x TSK 906 manual on USB stick
Ferrari F1 car in the pit lane surrounded by team members preparing for a pit stop, showcasing teamwork and racing action.

Consultancy & Sales

Do you have further questions about the instrument or the method and would like to speak to a sales representative?

Service & Support

Do you already have an instrument and need technical support or spare parts?

Downloads and Media

AI Overview
An error occurred. Please try again.