Simultaneous Thermal Analysis (STA)

based on, e.g., ISO 11358, ASTM E793, DIN 51004, DIN 51006, DIN 51007 

Simultaneous Thermal Analysis (STA) generally refers to the simultaneous application of Thermogravimetry (TGA) and Differential Scanning Calorimetry (DSC) to one and the same sample in a single instrument.

Detailed diagram of a Simultaneous Thermal Analysis (STA) instrument, highlighting components like gas supply, heating element, and sample carrier.

The advantages are obvious: 

The test conditions are perfectly identical for the TGA and DSC signals (same atmosphere, gas flow rate, vapor pressure on the sample, heating rate, thermal contact to the sample crucible and sensor, radiation effect, etc.). Furthermore, sample throughput Is improved as more information can be gathered from each test run.

DSC Possibilities

 

TGA Possibilities

Plastics: PET

Plastic bottles, textile fibers and films (for example, packaging for food) are well known applications of the polymer PET (polyethylene terephthalate). This STA measure-ment under nitrogen exhibits a step in the DSC signal below 100°C which is due to the Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.glass transition. A corresponding increase in specific heat of 0.35 J/(g·K) was detected. The EndothermicA sample transition or a reaction is endothermic if heat is needed for the conversion.endothermic DSC peak at 81°C is due to RelaxationWhen a constant strain is applied to a rubber compound, the force necessary to maintain that strain is not constant but decreases with time; this behavior is known as stress relaxation. The process responsible for stress relaxation can be physical or chemical, and under normal conditions, both will occur at the same time. relaxation, the ExothermicA sample transition or a reaction is exothermic if heat is generated.exothermic peak at 131°C is due to CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.crystallization and the EndothermicA sample transition or a reaction is endothermic if heat is needed for the conversion.endothermic peak at 255°C is due to melting. At temperatures above 360°C, the pyrolytic Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition of the sample occurred with a total mass loss of 79.5%.

Thermal analysis graph of PET sample showing TGA and DSC curves with key temperature points and mass loss data.
The SiC furnace was used for the investigation of the thermal behavior of a PET sample (10.13 mg) in a nitrogen atmosphere. The heating rate amounted to 10 K/min.