Easter cookie dough with various animal and flower-shaped cookie cutters, a rolling pin, and a sprinkle of flour on parchment paper.
differential scanning calorimetry

DSC 404 F3 Pegasus®

High-Temperature DSC up to 2000°C

Highlights

Fascinating Flexibility in Thermal Analysis 

The DSC 404 F3 Pegasus®, High-Temperature Differential Scanning Calorimeter, is part of the economical NETZSCH F3 -product line, which is specially tailored to the requirements of comparative material characterization and quality control.

The DSC 404 F3 Pegasus®, High-Temperature Differential Scanning Calorimeter, can be operated from -150°C to 2000°C with various DTA and DSC sensors that are easily exchangeable by the user and various furnace types (please see accessories).

The sample chamber can be purged with inert or oxidizing gases in order to remove gases evolved from the sample.

The measuring system is vacuum tight (10-4 mbar).

Method

The DSC 404 F1 as well as the F3 Pegasus® systems operate according to the heat flux principle. With this method, a sample and a reference are subjected to a controlled temperature program (heating, cooling or IsothermalTests at controlled and constant temperature are called isothermal.isothermal). The actual measured properties are the temperature of the sample and the temperature difference between sample and reference. From the raw data signals, the heat flow difference between sample and reference can be determined.

Schematic of a furnace setup for thermal analysis, depicting sample and reference positions with marked ΔT and heat flow (Q_P_R).
More on the Functional Principle of a Heat-Flux DSC

A DSC measuring cell consists of a furnace and an integrated heat-flux sensor with designated positions for the sample and reference pans.

The sensor areas are connected to thermocouples or may even be part of the thermocouple. This allows for recording both the temperature difference between the sample and reference side (DSC signal) and the absolute temperature of the sample or reference side.

Due to the heat capacity (cp) of the sample, the reference side (usually an empty pan) generally heats faster than the sample side during heating of the DSC measuring cell; i.e., the reference temperature (TR, green) increases a bit faster than the sample temperature (TP, red). The two curves exhibit parallel behavior during heating at a constant heating rate – until a sample reaction occurs. In the case shown here, the sample starts to melt at t1. The temperature of the sample does not change during melting; the temperature of the reference side, however, remains unaffected and continues exhibiting a linear increase. When melting is completed, the sample temperature also begins to increase again and, beginning with the point in time t2, again exhibits a linear increase.

The differential signal (ΔT) of the two temperature curves is presented in the lower part of the image. In the middle section of the curve, calculation of the differences generates a peak (blue) representing the EndothermicA sample transition or a reaction is endothermic if heat is needed for the conversion.endothermic melting process. Depending on whether the reference temperature was subtracted from the sample temperature or vice versa during this calculation, the generated peak may point upward or downward in the graphs. The peak area is correlated with the heat content of the transition (enthalpy in J/g).

Graph depicting thermocouple voltage vs. time, showing reference and sample signals, transition temperature, and enthalpy calculations.

Specifications

Technical Data

Temperature range
-150°C to 2000°C
Heating rates
(dependent on furnace)
0.001 K/min to 50 K/min
Measuring sensors
for DSC and DTA
NETZSCH analysis machine with two cylindrical chambers and a digital interface for precise material testing and analysis.

Thermocouple types:
S, E, K, B, W/Re, SProtected, P

Atmospheres:
inert, oxidizing, static, dynamic

Extension with unique OTS®® system
(option)

TypeTemperature rangeCooling system
Silver furnace-120°C to 675°Cliquid nitrogen
Copper furnace-150°C to 500°Cliquid nitrogen
Steel furnace -150°C to 1000°Cliquid nitrogen
Platinum furnaceRT to 1500°Cforced air
Silicon carbide furnaceRT to 1600°Cforced air
Rhodium furnaceRT to 1650°Cforced air
Graphite furnaceRT to 2000°Ctap or chilled water

Three magnetic valves with frits are available for reproducible gas flow. Optionally the system can be equipped with a mass flow controller.
A wide range of crucibles (pans) (aluminum, platinum, alumina, etc.) is available for nearly all possible applications and materials.
Complete sets of standards for metallic and ceramic sample containers are available for calibration of temperature and enthalpy values.
The concept allows for equipping a measuring instrument with a double-furnace hoisting device for two furnaces. The furnace can therefore be mounted on the double hoisting device combined with other furnaces.

Instead of a second furnace, an automatic sample changer (ASC) can optionally be used. Modular flexibility saves a great amount of time and thus directly results in an increased sample throughput. Optionally available, the OTS® system allows for reducing effectively the oxygen partial pressure at the sample vicinity.
The automatic sample changer (ASC) is designed for routine measurements. It works day and night, giving you time for other tasks, and provides for optimal use of the DSC 404 F3 Pegasus® (e.g. calibrations on the weekend).

A carousel is available for up to 20 sample and reference crucibles (pans) which can be automatically run in any order. The controlled generation of the required gas atmosphere in the sample chamber and cooling are automatic.
Of course, each sample can be assigned an individual measurement and evaluation macro. Easy-to-understand input masks lead you through the programming of the measurement series. And it is always possible to insert unplanned analyses into a preprogrammed series of measurements that is already in progress.

Round DSC sensor with dual thermocouple protection, ideal for precise temperature analysis in testing applications.
DSC sensor in round design, DSC sensor, DTA sensor with protected thermocouples
Detailed diagram of a gas analysis system, highlighting components like the heating element, thermocouple, and gas outlet valve.

PulseTA®

With the PulseTA® technique an exactly defined quantity of gas is injected to the purge gas of the thermobalance (TGA) or the simultaneous thermal analysis instrument (STA).

This clearly increases the measuring possibilities:

  • Defined/incremental chemical reactions or adsorption of the injection gas with the sample
  • Quantification of gases evolved from the sample.
Schematic of a gas analysis system showing injected and purge gas flow, pulse device, and monitoring components like TA and MS/FT-IR.

Crucibles (Pans) for the DSC 404 F1 /F3 Pegasus®

Material
(Purity)
Temperature
Range
Consisting ofDimension/
Volume
RemarksOrder Number
PtRh/Al2O3Max. 1700°CCrucible + liner + lidFor metal melts and other reactive materials 6.225.6-93.2.00
Al2O3 (99.7%)Max. 1700°CCrucible∅6.8mm/85µl GB399972
Al2O3 (99.7%)Max. 1700°CLid For GB399972GB399973
Pt/Rh (80/20)Max. 1700°CCrucible∅6.8mm/85µl GB399205
Pt/Rh (80/20)Max. 1700°CCrucible∅6.8mm/0.19mlHeight 6mmNGB801556
Al (99.5)Max. 600°CCrucible∅6.7mm/85µlSet of 100 piecesNGB810405
Al (99.5)Max. 600°CLid For NGB810405NGB810406
Gold (99.9)Max. 900°CCrucible + lid∅6.7mm/85µl  6.225.6-93.3.00
ZrO2Max. 2000°CCrucible85µlCaO-stabilizedGB397053
ZrO2Max. 2000°CLid For GB397053GB397052

* Please note: One and the same sealing press is capable of sealing all the Al crucibles (pan + lid), order no. 6.240.10-80.0.00A

Software

Proteus®: Excellent Thermal Analysis Software

The DSC 404 F3 Pegasus® runs under Proteus®Software on Windows®. The Proteus® Software includes everything you need to carry out a measurement and evaluate the resulting data. Through the combination of easy-to-understand menus and automated routines, a tool has been created that is extremely user-friendly and, at the same time, allows sophisticated analysis.The Proteus® software is licensed with the instrument and can of course be installed on other computer systems.

DSC features:

Further Advanced Software Options

The Proteus® modules and expert software solutions offer further advanced processing of the thermoanalytical data for more sophisticated analyses. 

Tau-R®Mode takes into account the time constant and thermal resistance of the instrument and reveals thus sharper DSC effects from the sample.

The DSC curve incorporates not only important information about the sample, but also residual information from the instrument. To correct for this established fact, the Tau‐R Mode has been developed. This method is based on two essential correction factors: the thermal resistance (R) and the time constant (τ). The determination and creation of a correction file need only be carried out once for identical measurement parameters. The true raw data can then be accessed by just one click of the mouse

Peak Separation permits accurate separation and evaluation of overlapping transitions. 

PeakSeparation allows for the presentation of experimental data in the form of the additive overlap­ping of peaks. This program offers different curve types such as Pearson, Gauß, Cauchy, etc.

Purity Determination is a program for determining the purity of a material through analysis of the DSC melting peak.

Prediction of Material Behavior and Reaction Processes:

Materials with accurately defined properties can be transformed into other substances with other properties by chemical reactions. The reactions can take place within a fraction of a second – like in the case of explosions – or take hundreds of thousands of years, as is the case in the formation of minerals. This is because processes like decomposition, curing, crystallization and sintering of materials are dependent on time and temperature. Knowledge about the speed of these processes is therefore important in order to simulate material behavior or optimize a process.

Kinetics, also called reaction kinetics or chemical kinetics, studies the rate of chemical processes and allows for determination of reaction rates. It also takes the factors, which control these reactions, into account.

NETZSCH Kinetics Neo software is used to analyze chemical processes. The software allows for the analysis of temperature-dependent processes. The result of such analysis is a kinetics model or method correctly describing experimental data under different temperature conditions. Use of the model allows for predictions of a chemical system’s behavior under user-defined temperature conditions. Alternatively, such models can be used for process optimization.

The software can analyze different types of thermal curves that depict the changes in a given material property measured during a process. Potential data sources include studies using Differential Scanning Calorimetry (DSC), Thermogravimetry (TGA), Dilatometry (DIL), Dielectric Analysis (DEA), Accelerating Rate Calorimetry (ARC)The method describing isothermal and adiabatic test procedures used to detect thermally exothermic decomposition reactions.Accelerating Rate Calorimetry (Accelerating Rate Calorimetry (ARC)The method describing isothermal and adiabatic test procedures used to detect thermally exothermic decomposition reactions.ARC®), Rheology and Viscosity (Torque).

Ferrari F1 car in the pit lane, surrounded by mechanics preparing for a quick tire change during a race.

Consultancy & Sales

Do you have further questions about the instrument, the method and would you like to speak to a sales representative?

Service & Support

Do you already have an instrument and need technical support or spare parts?

AI Overview
An error occurred. Please try again.