Seminar
Circular Economy of Plastics: Tools to Identify and Analyse Unknown Compositions
Program
| 16:30 - 16:35 | Welcome & Introduction to NETZSCH | Andrew Gillen |
| 16:35 - 16:50 | Circular Economy of Plastics: Recycling challenges and identifying unknown polymer compositions | |
| 16:50 - 17:00 | DSC for Polymer Identification: Introduction and measurement principle | Dr. Markus Meyer |
| 17:00 - 17:20 | Live SMART MODE DSC Measurement – PE/PP: Sample preparation, loading and starting the measurement | |
| 17:20 - 17:40 | Identifying & Quantifying Unknown Polymer Mixtures: DSC identification, PE/PP mixtures and peak separation | Andrew Gillen |
| 17:40 - 18:00 | Return to the Live PE/PP Measurement: Evaluation, Interpretation and Key Takeaways | Dr. Markus Meyer |
| 18:00 - 18:30 | Q&A and Wrap Up |