16.08.2022 by Aileen Sammler

Expandable Graphite: A Sustainable Solution for Flame Retardants in Plastics

Burning laptop in flames showcases the urgency of effective flame retardants like expandable graphite in plastics.

Flame retardants (FRs) have been used for decades to reduce or even eliminate the risk of fire hazards in plastic components for such applications as the electronics or automotive industries. Expandable graphite, which most only associate with increased thermal and Electrical Conductivity (SBA)Electrical conductivity is a physical property indicating a material's ability to allow the transport of an electric charge.electrical conductivity, can also be utilized to increase fire safety.

Flame retardants (FRs) have been used for decades to reduce or even eliminate the risk of fire hazards in plastic components for such applications as the electronics or automotive industries. The most important initiative right now is the EU’s Green Deal, which will result in strong opportunities and, potentially, obligations to transition to halogen-free FRs. This will be even more likely when the anticipated revision of the RoHS (Restriction of Hazardous Substances) takes place.

There is a variety of different solutions and numerous FR polymers available on the market. One of them is expandable graphite, which most only associate with increased thermal and Electrical Conductivity (SBA)Electrical conductivity is a physical property indicating a material's ability to allow the transport of an electric charge.electrical conductivity. Its unique properties can also be utilized to increase fire safety.

NETZSCH Taurus Cone Calorimeter TCC 918 for flame retardant testing, featuring a digital interface and smoke measurement capabilities.
Figure: NETZSCH Taurus Cone Calorimeter TCC 918

 

 

 

To highlight the effect of different amounts of expandable graphite as a flame retardant on the fire behavior of polyethylene, samples of the different compounds were injection-molded and tested in the NETZSCH Taurus Cone Calorimeter TCC 918. 

The instrument allows for the determination of the heat release, mass loss and DensityThe mass density is defined as the ratio between mass and volume. density and composition of the smoke gas.

This study shows that expandable graphite is a suitable flame retardant for polyethylene (PE) and that, within the range of FR content levels investigated here, it is possible to increase the effect by using higher amounts of FR.

 

Please find more information about the Cone Calorimeter TCC 918 on our website.

 