Published on 

Penetration Model in the NETZSCH LFA Software − Porous Materials Finally Handled Properly!

Introduction

Since the development of the laser flash method by Parker et al. in 1961 [1], various improvements have been made to this method for the non-contact, non-destructive determination of the Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.thermal diffusivity. Nowadays, hardware and software should allow for measurements on different sample geometries, shapes and forms. It became necessary for the laser/light flash apparatus (LFA) to be able to test not only solids, but also powdery, liquid, crumbled and porous specimens. For this reason, certain hardware prerequisites such as specific sample holders must be provided. In addition, software models that consider the influence of the shape and form of the specimen are becoming increasingly important for the precise determination of the Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.thermal diffusivity (a), Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity (λ) and Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.specific heat capacity (cp). 

In recent years, NETZSCH has continuously improved and developed calculation models, corrections and mathematical operations taking into account heat loss in combination with pulse correction, radiation, multilayer systems, in-plane tests, baseline corrections, etc. This application note presents the Penetration model based on McMasters [2] for measurements on porous materials.

Porous Materials Are a Challenge – But Not for the Penetration Model

For standard flash measurements, the front face of the specimen absorbs the total energy. A thermal wave will then travel through the specimen’s thickness before reaching the rear face (figure 1). For porous materials, NETZSCH has now introduced the Penetration model (figure 2) that includes the following considerations: 

  • Absorption of the pulse energy is no longer limited to the front face 
  • Absorption is extended over a thin layer into the specimen's thickness 
  • Absorption layers can be handled as the mean free path in the material 

Taking these aspects into account results in an exponentially decaying initial temperature distribution within the specimen. Applying this approach, which accounts for the porosity of the material, results in improved accuracy and precision of the Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.thermal diffusivity, Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity and Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.specific heat capacity values determined.

LFA method diagram illustrating components: detector, furnace, sample thermocouple, power source, and heating element.
1) Diagram of LFA method
Schematic diagram illustrating the penetration model in NETZSCH Proteus LFA software, showcasing directional arrows and key terminology.
2) Penetration model implemented in the NETZSCH Proteus® LFA software

Measurement Conditions

A graphite felt insulation was measured between room temperature and 90°C with the NETZSCH LFA 427 and, for purposes of comparison, with the NETZSCH heat flow meter HFM 436 Lambda. The specimen thicknesses amounted to 5.4 mm and 20 mm, respectively. The DensityThe mass density is defined as the ratio between mass and volume. density was determined to be 0.082 g/cm3 at 20°C.

Measurement Results

Figure 3 depicts: a) the LFA measurement results demonstrating the course of the monitored Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.thermal diffusivity based on the Penetration model, b) the literature data of the Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.specific heat capacity of POCO graphite, and c) the calculated Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity based on the equation: 

λ = а · ρ · cp 

with 
λ = Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity 
α = Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.thermal diffusivity 
ρ = DensityThe mass density is defined as the ratio between mass and volume. density 
cp = Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.specific heat capacity 

The LFA measurement was first evaluated with the standard model (Cowan, [3]) and a second time with the Penetration model. Figure 4 clearly shows that the same measurement yields different Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity results when using different calculation models. The question as to which is the better result can be answered by checking the signal increase (figure 5). 

Figure 5 shows the rise of the detector signal. The left plot depicts the use of the standard model. It clearly indicates that the standard model yields an insufficient model fit. In this case, the thermal diffusivity is determined to be 0.753 mm2/s – a value too high for the investigated material. However, an excellent model fit results when using a fit based on the Penetration model (right plot). The resulting thermal diffusivity value, a = 0.626 mm2/s, is approximately 17% lower and, due to the improved fit, far more reliable than the one achieved with the standard Cowan model. 

The thermal conductivity is proportional to the thermal diffusivity and therefore the values are higher for standard materials, too. The reliability of the results obtained with the Penetration model is confirmed by HFM measurements on the same material. LFA and HFM results are in good agreement; the maximum deviation is less than ±6% (figure 6).

LFA measurement graph showcasing thermal diffusivity, conductivity, and specific heat capacity of Poco graphite with varying temperatures.
3) LFA measurement on the graphite felt insulation along with literature data on the Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.specific heat capacity for Poco graphite
Graph comparing thermal conductivity models (Cowan vs. Penetration) for graphite felt insulation across temperatures.
4) LFA measurement on the graphite felt insulation along with literature data on the specific heat capacity for Poco graphite
Laser speed comparison graphs: standard model shows 0.753 mm²/s, while laser penetration model shows 0.626 mm²/s, 17% lower.
5) left: Laser shot without penetration: 0.753 mm²/s, right: Laser shot with penetration: 0.626 mm²/s
Thermal conductivity graph comparing LFA (standard and penetration models) and HFM results across temperature ranges.
6) Thermal conductivity determined by means of LFA using the standard and Penetration models(red curve) and HFM (blue curve)

Conclusion

Along with the various classical models (e.g., Cowan 5 / 10, Parker, improved Cape-Lehman, etc.), the NETZSCH LFA Proteus® software includes many different calculation models, corrections and mathematical operations. One of them is the Penetration model, which is suitable specifically for porous materials and materials with a rough surface. This special feature of the LFA Proteus® software involves the penetration of the light flash into the specimen beyond the actual heated surface. It accounts for the specimen’s porosity, which causes a portion of the light flash energy to be deposited inside the specimen. This means the Penetration model takes into account absorption of the pulse energy over a thin layer into the specimen’s thickness. Other reliable methods such as Heat Flow Meter (HFM) confirm the LFA results obtained by applying the Penetration model for calculation of the thermal diffusivity/conductivity.

Literature

  1. [1]
  2. [2]
  3. [3]
    Cowan, Robert D.; Journal of Applied Physics, Vol. 34, Number 4 (Part 1), April 1963