Shear Thinning

The most common type of Non-NewtonianA non-Newtonian fluid is one that exhibits a viscosity that varies as a function of the applied shear rate or shear stress.non-Newtonian behavior is shear thinning or pseudoplastic flow, where the fluid vis­cosity decreases with increasing shear. 

At low enough shear rates, shear thinning fluids will show a constant viscosity value, η0, termed the zero-shear viscosity or zero- shear viscosity plateau. At a critical shear rate or shear StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress, a large drop in viscosity is observed which signi­fies the beginning of the shear thinning region. At very high shear rates, a second constant viscosity plateau is observed, called the infinite shear viscosity plateau. This is given the symbol η∞and can be several orders of mag­nitude lower than η0depending on the degree of shear thinning.

Graph illustrating shear thinning behavior, displaying viscosity decreases across shear rates, with labels for zero-shear and infinite shear plateaus.

Do you have any questions?

Our experts will be happy to help you.

Contact us

Suitable products for your measurement

AI Overview
An error occurred. Please try again.