Unlocking the Pyrolysis of Olive Stone Biomass: TGA Analysis and the Appropriate Kinetic Approach

Introduction

PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.Pyrolysis has emerged as a key thermochemical process in the transition toward sustainable and circular energy systems. It enables the conversion of a wide range of carbon-based feedstocks into valuable fuels, chemicals, and carbon-rich solids. 

Among the various materials suitable for PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis are biomass and organic waste, plastics, and rubber-based materials like waste tires. These feedstocks offer different end products, from biochar and syngas to fuels and industrial carbon materials depending on their composition and processing conditions. 

Focusing on biomass as a renewable resource has significant potential in biofuel production and the generation of value-added chemicals. The conversion of biomass through processes such as PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis, gasification, and combustion offers sustainable solutions to meet the growing demand for energy [1]. Among the various biomass feedstocks, olive stones stand out as a particularly valuable resource [2]. A byproduct of the olive industry, olive stones possess high energy potential due to their low moisture content and rich lignocellulosic composition. These characteristics make olive stones ideal for biofuel production through PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis. Also, olive stones can be converted into biochar, activated carbon, and biochemicals, offering diverse applications beyond energy production. 

This study focuses on the PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis kinetics of olive stone biomass. Based on thermogravimetric measurements, a comprehensive kinetic analysis of olive stone biomass is performed using the NETZSCH Kinetics Neo software to determine key kinetic parameters and perform process optimization through simulation.

Measurement Conditions

The measurement condition are detailed in table 1. The TGA curves obtained are the basis for kinetic evaluation of the Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition reaction.

Table 1: Thermogravimetric analysis (TG) test parameters

InstrumentNETZSCH TG 309 Classic
CrucibleAl2O3, open
Sample mass9.65 mg to 9.85 mg
Temperature range25°C to 1000°C
AtmosphereNitrogen (40 ml/min), switch to synthetic air (40 ml/min) at 900°C
Heating rates2.5 K/min, 5 K/min, 7.5 K/min, 10 K/min, 15 K/min, 20 K/min,

Measurement Results

The TGA measurements in figure 1 depict the TGA and DTG (first derivative) curves of the measurements on olive stone at heating rates of 2.5, 5, 7.5, 10, 20, 30 and 40 K/min under an inert atmosphere. The first mass-loss step, detected between room temperature and 130°C, results from moisture evaporation and is accompanied by a mass loss of 3.3% [3]. After the dehydration process, several overlapped mass-loss steps take place at temperatures between 130°C and 700°C, attributed to the thermal degradation of hemicellulose; this is followed by cellulose degradation, and finally a prolonged mass loss, which might be attributed to the degradation of lignin [4]. The mass losses observed at temperatures above 700°C are due to the thermal degradation of resilient lignin structures [5]. They are shifted to higher temperatures with increasing heating rates (kinetic influence) [6].

TGA and DTG curves for olive stone analysis across various heating rates, showing weight changes from 200 to 1000°C.
1) TGA measurement on olive stone at different heating rates; solid lines: TGA, dashed lines: DTG

Kinetic Analysis of Thermal Decomposition

Using the NETZSCH Kinetics Neo software, the dependence of the Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition process on the heating rate can be evaluated. The TGA profile for the rate of 40 K/min is depicted in figure 2. This observation indicates that the PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis process is not fully completed by 700°C, but rather proceeds gradually up to 900°C, accompanied by a mass loss. The initial mass-loss step prior to 140°C, which pertains to the removal of moisture, was not taken into account in the data that was subjected to kinetic analysis [3]. When switching from nitrogen to oxygen at 900°C, a mass loss occurs due to combustion. This data was excluded from the kinetic analysis. Figure 2 shows the TGA measurement curves between 130°C and 900°C used for the kinetic evaluation.

TGA data graph showing the mass decrease of olive stone decomposition at various heating rates from 100°C to 900°C.
2) Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. Decomposition of olive stone to 900°C at different heating rates, measured TGA data

The degree of conversion, α, is calculated by Kinetics Neo software from thermogravimetry measurements where α ranges from 0 to 1 (Eq 1).

Equation representing the analysis of mass loss, highlighting variables m0, mt, and m∞ in material testing.

m0: initial mass
mt: mass at time t
m∞: final mass

Due to the complexity of biomass, a detailed understanding of reaction kinetics is essential for designing efficient reactors and optimizing process conditions [8]. The PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis of hemicellulose begins at a relatively low temperature (~200°C) [9]. Cellulose Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition involves multiple steps, including the formation of an amorphous intermediate and the production of levoglucosan [10]. Lignin is the most stable component due to its aromatic ring structure, with Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition occurring over a temperature range from 170°C to the end of the process [3].

The thermal Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition of olive stone occurs in multiple stages, as illustrated in figure 3, where the conversion rate is defined as the first derivative of conversion with respect to time. The first shoulder at 198°C marks the early Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition of hemicellulose, followed by its main Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition phase around 260°C. The primary breakdown of cellulose occurs at the main peak near 306°C with a late Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition stage at 340°C. Finally, lignin decomposes slowly, showing a final shoulder at 384°C. [7]

This suggests a multi-step reaction process, which can be modeled with a five-step kinetic model:

A → B → C → D → E

F → G

The reaction rate of each step, j, is described by the function (Eq 2):

Reaction Rate j = Aj · f(ej, pj) · exp (-Ej/(RT)) (Eq 2)

Aj: pre-exponential factor

Ej: activation energy [J/mol]

T: temperature [K]

R: gas constant (8.314 J/K.mol)

f (ej ,pj): function dependent on the concentration of the initial reactant, ej, and the concentration of product, pj

Conversion rate graph showing a peak at 306°C and four shoulders, indicating a five-step decomposition process.
3) Conversion rate of the measurement at 2.5 K/min to 700°C. One peak and 4 shoulders indicate a 5-step Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition process.

The thermal Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition of the olive stone can be fitted by five peaks, corresponding to the sum of peaks at temperatures 198°C, 260°C, 306°C, 340°C, and 384°C, as shown in figure 4. These peaks represent the sequential Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition of hemicellulose, cellulose, and lignin during the PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis process [6].

Graph depicting conversion rates (%) per minute against temperature (°C), highlighting a 5-step decomposition process with key peaks and shoulders.
4) Conversion rate of the measurement at 5 K/min to 700°C. One peak, and 4 shoulders indicate a 5-step decomposition process.

The measured data is presented as arhombus line, the thick green curve is the sum of the individual reaction steps. The good agreement between experimental and simulated data confirms the assumption of a 5-step process.

Figure 5 shows the measured TGA curves as well as the curves calculated using the five-step kinetics model in the NETZSCH Kinetics Neo software. Table 2 summarizes the parameters of the kinetics. The results demonstrate strong agreement between the measured and calculated data, with a coefficient of determination of 0.999.

Kinetic evaluation graph showing olive stone decomposition with mass percentage versus temperature curves and measured data points.
5) Kinetic evaluation of the decomposition of olive stone. Rhombus lines: measured curves; solid lines: calculated curves based on a five-step reaction.

Table 2: Kinetic parameters of the thermal degradation of olive stone

Reaction step

A → B

Fn1

B → C

Fn1

C → D

Fn1

D → E

Fn2

F → G

DFn2

Activation energy [kJ/mol]151.824165.479194.592206.720179.468
Log (Pre-Exp) Log (1/s)14.08313.79215.11615.28612.093
Reaction order1.8322.7321.0391.4666.304
Contribution0.0610.3360.3130.0730.217
Coefficient of determination0.999

1Fn: Reaction ofnth order
2DFn: One-dimensional diffusion ofnth order

Simulation: Process Optimization

Following kinetic analysis and the determination of all relevant kinetic parameters, the next step involves process optimization as shown in figures 6 and 7. At this stage, the goal is to control the decomposition process by adjusting the conversion rate in order to minimize the total time required to achieve the desired conversion. Figure 7 presents the temperature program and time for a 2.5%/min conversion rate, corresponding to the simulated conversion rate.

Optimized temperature program and mass loss curve illustrate conversion rate control over time in testing processes.
6) Optimized temperature program (dashed line) for control of the constant mass loss 2.5%/min of the conversion rate, and mass loss curve (solid line) for this temperature program.
Analysis results for "PEI-PTFE Ultem 4001" show its top similarity score of 100% among materials listed.
7) Conversion rate (2.5%/min) vs. time for process optimization; convesion rate (solid line) and temperature (dashed line).

Conclusion

A comprehensive kinetic analysis can be conducted by combining NETZSCH TGA measurements with the NETZSCH Kinetics Neo software. The resulting determination of kinetic parameters allows for process optimization, enhancing overall efficiency and minimizing the total time required to achieve the desired conversion. Accurate kinetic parameters are essential for designing efficient reactors that enhance overall process performance. This approach can be applied to a wide range of feedstock materials such as biomass, plastics, and rubber.

Literature

  1. [1]
    Wang S., Dai G., Yang H., & et al. (2017). Lignocellulosic biomass PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis mechanism: A state-of-the-art review. Progress in Energy and Combustion Science, 62, 33–86.
  2. [2]
    García Martín, J. F., Cuevas, M., Feng, C. H., Mateos, P. Á., García, M. T., & Sánchez, S. (2020). Energetic valorisation of olive biomass: Olive-tree pruning, olive stones and pomaces. In Processes (Vol. 8, Issue 5).https://doi.org/10.3390/PR8050511
  3. [3]
    Asimakidou, T., & Chrissafis, K. (2022). Thermal behavior and PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis kinetics of olive stone residue. Journal of Thermal Analysis and Calorimetry, 147(16).
    https://doi.org/10.1007/s10973-021-11163-w
  4. [4]
  5. [5]
    Sanginés, P., Domínguez, M. P., Sánchez, F., & San Miguel, G. (2015). Slow PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis of olive stones in a rotary kiln: Chemical and energy characterization of solid, gas, and condensable products. Journal of Renewable and Sustainable Energy, 7(4).
    https://doi.org/10.1063/1.4923442
  6. [6]
    Moukhina, E. (2012). Determination of kinetic mechanisms for reactions measured with thermoanalytical instruments. Journal of Thermal Analysis and Calorimetry, 109(3). 
    https://doi.org/10.1007/s10973-012-2406-3
  7. [7]
    Marcilla, A., García, A. N., Pastor, M. v., León, M., Sánchez, A. J., & Gómez, D. M. (2013). Thermal decomposition of the different particles size fractions of almond shells and olive stones. Thermal behaviour changes due to the milling processes. Thermochimica Acta, 564. 
    https://doi.org/10.1016/j.tca.2013.04.019
  8. [8]
    SriBala, G., Carstensen, H. H., van Geem, K. M., & Marin, G. B. (2019). Measuring biomass fast PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis kinetics: State of the art. In Wiley Interdisciplinary Reviews: Energy and Environment (Vol. 8, Issue 2). John Wiley and Sons Ltd. https://doi.org/10.1002/wene.326
  9. [9]
    Zhou, H., Long, Y., Meng, A., Chen, S., Li, Q., & Zhang, Y. (2015). A novel method for kinetics analysis of PyrolysisPyrolysis is the thermal decomposition of organic compounds in an inert atmosphere.pyrolysis of hemicellulose, cellulose, and lignin in TGA and macro-TGA. RSC Advances, 5(34), 26509–26516.https://doi.org/10.1039/c5ra02715b
  10. [10]
    Burnham, A. K., Zhou, X., & Broadbelt, L. J. (2015). Critical review of the global chemical kinetics of cellulose thermal decomposition. In Energy and Fuels (Vol. 29, Issue 5, pp. 2906–2918). American Chemical Society. https://doi.org/10.1021/acs.energyfuels.5b00350
AI Overview
An error occurred. Please try again.